Cargando…
Bus bar joints stability and protection
A defective bus connection between two dipole magnets was the primary cause of the incident in sector 34 on September 19th. I will show how this could have happened, i.e. how a highly resistive joint has caused a thermal runaway and burned (or opened) before the QPS threshold was reached. In the sec...
Autor principal: | Verweij, A |
---|---|
Lenguaje: | eng |
Publicado: |
2009
|
Materias: | |
Acceso en línea: | http://cds.cern.ch/record/1172401 |
Ejemplares similares
-
Measurement of the Residual Resistivity Ratio of the Bus Bars Copper Stabilizer of the 13 kA Circuits of the LHC
por: Apollonio, A, et al.
Publicado: (2012) -
Heat Transfer in the LHC Main Superconducting Bus Bars
por: Granieri, P P, et al.
Publicado: (2011) -
Development of an enhanced dielectric insulation for the PS Bus Bars
por: Bodart, Dominique
Publicado: (2012) -
Non-Destructive Testing of Bus-Bar Joints Powering LHC Superconducting Magnets, by Using Gamma Sources
por: Skoczen, B, et al.
Publicado: (2004) -
The high current bus-bars of the LHC from conception to manufacture
por: Belova, L, et al.
Publicado: (2006)