Cargando…
Production of Cs and Fr isotopes from a high density UC targets with different grain dimensions
A UC target material of 12 g/cm3 density with the grain size of 20 and 5 μm manufactured in a form of pills by the method of powder metallurgy has been tested on-line within the temperature range of (1800-2000) °C. Abstract to ENAM2008
Autores principales: | Panteleev, V. N, Volkov, Yu. M, Barzakh, A. E, Fedorov, D. V, Ivanov, V. S, Mezilev, K. A, Moroz, F. V, Molkanov, P. L, Alyakrinskiy, O, Barbui, M, Tonezzer, M, Stroe, L, Orlov, S. Yu, Tecchio, L. B, Lhersonneau, G |
---|---|
Lenguaje: | eng |
Publicado: |
30/0
|
Materias: | |
Acceso en línea: | http://cds.cern.ch/record/1356490 |
Ejemplares similares
-
Influence of radiative filiation on measured release curves
por: Lhersonneau, G, et al.
Publicado: (2006) -
Influence of decay in the target on the measurement of release times and release efficiency
por: Lhersonneau, G, et al.
Publicado: (2008) -
Studies of uranium carbide targets of a high density
por: Panteleev, V N, et al.
Publicado: (26/0) -
Electron beam - plasma ionizing target for production of neutron-rich nuclides
por: Panteleev, V.N, et al.
Publicado: (15/0) -
Test of high density UC targets development at Gatchina for neutron rich radioactive beam facilities
por: Lhersonneau, G, et al.
Publicado: (2008)