Cargando…
Saturation behaviour of the LHC NEG coated beam pipes
In the CERN Large Hadron Collider (LHC), about 6 km of the UHV beam pipe are at room temperature and serve as experimental or utility insertions. TiZrV non-evaporable getter (NEG) coating is used to maintain the design pressure during beam operation. Molecular desorption due to dynamic effects is st...
Autores principales: | Porcelli, T, Bregliozzi, G, Lanza, G, Baglin, V, Jimenez, J M |
---|---|
Lenguaje: | eng |
Publicado: |
2012
|
Materias: | |
Acceso en línea: | http://cds.cern.ch/record/1470599 |
Ejemplares similares
-
Evaluation of the NEG Coating Saturation Level after 3 Years of LHC Beam Operation
por: Bregliozzi, G, et al.
Publicado: (2013) -
LHC Experimental Beam Pipe Upgrade during LS1
por: Lanza, G, et al.
Publicado: (2014) -
Measurement of NEG Coating Performance Variation in the LHC after the First Long Shutdown
por: Bencini, Vittorio, et al.
Publicado: (2015) -
LHC Beam Vacuum During 2011 Machine Operation
por: Lanza, G, et al.
Publicado: (2012) -
CERN Vacuum-System Activities during the Long Shutdown 1: The LHC Beam Vacuum
por: Baglin, V, et al.
Publicado: (2014)