Radioactivity of Nb$_{3}$Sn/Cu wires after proton irradiation

Superconducting magnets based on Nb$_{3}$Sn technology are being developed for the LHC high luminosity upgrade. In this context irradiation induced changes of the superconducting properties of state-of-the-art Ti and Ta doped Nb$_{3}$Sn wires are presently studied. During irradiation tests with prot...

Descripción completa

Detalles Bibliográficos
Autores principales: Otto, Th, Scheuerlein, C, Catherall, R, Glaser, M, Militaru, O, Flükiger, R, Ballarino, A, Bottura, L
Lenguaje:eng
Publicado: 2013
Materias:
Acceso en línea:https://dx.doi.org/10.1109/TASC.2012.2233263
http://cds.cern.ch/record/1516050
_version_ 1780928431061467136
author Otto, Th
Scheuerlein, C
Catherall, R
Glaser, M
Militaru, O
Flükiger, R
Ballarino, A
Bottura, L
author_facet Otto, Th
Scheuerlein, C
Catherall, R
Glaser, M
Militaru, O
Flükiger, R
Ballarino, A
Bottura, L
author_sort Otto, Th
collection CERN
description Superconducting magnets based on Nb$_{3}$Sn technology are being developed for the LHC high luminosity upgrade. In this context irradiation induced changes of the superconducting properties of state-of-the-art Ti and Ta doped Nb$_{3}$Sn wires are presently studied. During irradiation tests with protons of 65 MeV at the cyclotron of Université Catholique de Louvain (UCL), 1.4 GeV at the CERN ISOLDE facility, and 24 GeV at the CERN IRRAD1 facility, the superconductor samples become radioactive and their handling must follow the legal specifications for radioactive materials. We have estimated the activation and the resulting ambient dose equivalent rate up to a fluence of 1017 p/cm2 with the Monte-Carlo Code FLUKA. The estimates were verified with experimental activation spectra. Samples for magnetization measurements with a mass of approximately 20 mg have to be considered as radioactive, but they do not have the potential to harm the operators handling them at radiation levels below 1 uSv/h. Larger samples (longer wires and sample holder materials like Cu and TiAl6V4) show correspondingly higher ambient dose equivalent rates and activation levels and they must be handled by radiation workers in designated areas, taking into account the standard precautions for work with radioactive materials. The use of radiation shielding during handling is recommended.
id cern-1516050
institution Organización Europea para la Investigación Nuclear
language eng
publishDate 2013
record_format invenio
spelling cern-15160502019-09-30T06:29:59Zdoi:10.1109/TASC.2012.2233263http://cds.cern.ch/record/1516050engOtto, ThScheuerlein, CCatherall, RGlaser, MMilitaru, OFlükiger, RBallarino, ABottura, LRadioactivity of Nb$_{3}$Sn/Cu wires after proton irradiationAccelerators and Storage RingsSuperconducting magnets based on Nb$_{3}$Sn technology are being developed for the LHC high luminosity upgrade. In this context irradiation induced changes of the superconducting properties of state-of-the-art Ti and Ta doped Nb$_{3}$Sn wires are presently studied. During irradiation tests with protons of 65 MeV at the cyclotron of Université Catholique de Louvain (UCL), 1.4 GeV at the CERN ISOLDE facility, and 24 GeV at the CERN IRRAD1 facility, the superconductor samples become radioactive and their handling must follow the legal specifications for radioactive materials. We have estimated the activation and the resulting ambient dose equivalent rate up to a fluence of 1017 p/cm2 with the Monte-Carlo Code FLUKA. The estimates were verified with experimental activation spectra. Samples for magnetization measurements with a mass of approximately 20 mg have to be considered as radioactive, but they do not have the potential to harm the operators handling them at radiation levels below 1 uSv/h. Larger samples (longer wires and sample holder materials like Cu and TiAl6V4) show correspondingly higher ambient dose equivalent rates and activation levels and they must be handled by radiation workers in designated areas, taking into account the standard precautions for work with radioactive materials. The use of radiation shielding during handling is recommended.CERN-ATS-2013-023oai:cds.cern.ch:15160502013-02-14
spellingShingle Accelerators and Storage Rings
Otto, Th
Scheuerlein, C
Catherall, R
Glaser, M
Militaru, O
Flükiger, R
Ballarino, A
Bottura, L
Radioactivity of Nb$_{3}$Sn/Cu wires after proton irradiation
title Radioactivity of Nb$_{3}$Sn/Cu wires after proton irradiation
title_full Radioactivity of Nb$_{3}$Sn/Cu wires after proton irradiation
title_fullStr Radioactivity of Nb$_{3}$Sn/Cu wires after proton irradiation
title_full_unstemmed Radioactivity of Nb$_{3}$Sn/Cu wires after proton irradiation
title_short Radioactivity of Nb$_{3}$Sn/Cu wires after proton irradiation
title_sort radioactivity of nb$_{3}$sn/cu wires after proton irradiation
topic Accelerators and Storage Rings
url https://dx.doi.org/10.1109/TASC.2012.2233263
http://cds.cern.ch/record/1516050
work_keys_str_mv AT ottoth radioactivityofnb3sncuwiresafterprotonirradiation
AT scheuerleinc radioactivityofnb3sncuwiresafterprotonirradiation
AT catherallr radioactivityofnb3sncuwiresafterprotonirradiation
AT glaserm radioactivityofnb3sncuwiresafterprotonirradiation
AT militaruo radioactivityofnb3sncuwiresafterprotonirradiation
AT flukigerr radioactivityofnb3sncuwiresafterprotonirradiation
AT ballarinoa radioactivityofnb3sncuwiresafterprotonirradiation
AT bottural radioactivityofnb3sncuwiresafterprotonirradiation