Coupling Current and Hysteresis Losses of Bi2212 Round Wires with Twisted Filaments
AC loss measurements have been carried out on Bi2212 round wires of different twist pitches. With systematical variation of sample temperature (5 K – 70 K) and ac field amplitude (≤0.2 T) as well as frequency (20 Hz – 2 kHz), this work shows (a) the full coupling of the non-twisted wire, (b) the unc...
Autores principales: | Yang, I, Pelegrin, J, Young, EA, Falorio, I, Ballarino, A, Bottura, L, Miao, H, Huang, Y |
---|---|
Lenguaje: | eng |
Publicado: |
2015
|
Materias: | |
Acceso en línea: | https://dx.doi.org/10.1109/TASC.2014.2373655 http://cds.cern.ch/record/1987560 |
Ejemplares similares
-
Strain induced irreversible critical current degradation in highly dense Bi-2212 round wire
por: Bjoerstad, R, et al.
Publicado: (2015) -
Synchrotron Microtomography Investigation of the Filament Microstructure in Differently Processed Bi-2212 Wires
por: Scheuerlein, Christian, et al.
Publicado: (2017) -
Reduction of Gas Bubbles and Improved Critical Current Density in Bi-2212 Round Wire by Swaging
por: Jiang, J, et al.
Publicado: (2013) -
Influence of the oxygen partial pressure on the phase evolution during Bi-2212 wire melt processing
por: Scheuerlein, C., et al.
Publicado: (2016) -
Processing of Bi-2212 high temperature superconducting wires
por: Doerrer, Christopher
Publicado: (2019)