Cargando…
One long tie bar broken after 3 days because of hydrogen contamination.
The tie bars have been produced with a high yield strength. As known for these type of high strength bolts, and hydrogen contamination during manufacture or heat treatment could lead to rupture under stress after several days.
Autor principal: | H. Gerwig |
---|---|
Publicado: |
2000
|
Materias: | |
Acceso en línea: | http://cds.cern.ch/record/41254 |
Ejemplares similares
-
Intergranular decohesion due to hydrogen contamination in barrel tie bars.
Publicado: (2000) -
Measurement of the location of tie-bar shoulders
por: Hubert Gerwig
Publicado: (2001) -
Test to rupture of titanium tie-bars for the coil suspension.
por: Saclay
Publicado: (2000) -
Broken tongue of cabling machine
por: S. Horvath
Publicado: (2000) -
Broken filaments in Rutherford cable
por: S. Horvath
Publicado: (2000)