Cargando…

Influence of the surface treatment of the CMS conductor on its adhesion properties at 300 K and 4.2 K

In the 4 T, 12.5 m long, 6 m bore diameter superconducting solenoid for the compact muon solenoid (CMS) experiment at large hadron collider (LHC), the interfaces between the insulation and the conductor or the external cylinder are subjected to high shear forces during the cool down to 4.5 K and the...

Descripción completa

Detalles Bibliográficos
Autores principales: Rondeaux, F, Kircher, F, Levesy, B, Reytier, M, Safrany, J S
Lenguaje:eng
Publicado: 2001
Materias:
Acceso en línea:https://dx.doi.org/10.1016/S0921-4534(01)00143-5
http://cds.cern.ch/record/508317

Ejemplares similares