Radiation-hardness studies of high OH**- content quartz fibres irradiated with 500 MeV electrons
We investigated the darkening of nine high OH**- fibre types irradiated with 500 MeV electrons from the Linac Injector of LEP (LIL) at CERN. The transmission of Xe light was measured in situ in the 350-800 nm range. The induced attenuation at 450 nm is typically 1.52 plus or minus 0.15 dB/m for a 10...
Autores principales: | , , , , , , , , , , , , , , |
---|---|
Lenguaje: | eng |
Publicado: |
2002
|
Materias: | |
Acceso en línea: | https://dx.doi.org/10.1016/S0168-9002(02)01067-7 http://cds.cern.ch/record/597182 |
_version_ | 1780899896754176000 |
---|---|
author | Merlo, J P Dumanoglu, I Akchurin, N Akgun, U Ayan, S Brücken, P Eskut, E Fenyvesi, A Kayis-Topaksu, A Koca, N Makónyi, K Novák, D Önel, Y M Onengüt, G Polatoz, A |
author_facet | Merlo, J P Dumanoglu, I Akchurin, N Akgun, U Ayan, S Brücken, P Eskut, E Fenyvesi, A Kayis-Topaksu, A Koca, N Makónyi, K Novák, D Önel, Y M Onengüt, G Polatoz, A |
author_sort | Merlo, J P |
collection | CERN |
description | We investigated the darkening of nine high OH**- fibre types irradiated with 500 MeV electrons from the Linac Injector of LEP (LIL) at CERN. The transmission of Xe light was measured in situ in the 350-800 nm range. The induced attenuation at 450 nm is typically 1.52 plus or minus 0.15 dB/m for a 100 Mrad absorbed dose. Two- parameter fits for darkening and recovery are presented. After irradiation the tensile strength remains essentially unchanged. For Polymicro quartz core fibres the tensile strength is typically 4.6 plus or minus 0.4 GPa. |
id | cern-597182 |
institution | Organización Europea para la Investigación Nuclear |
language | eng |
publishDate | 2002 |
record_format | invenio |
spelling | cern-5971822019-09-30T06:29:59Zdoi:10.1016/S0168-9002(02)01067-7http://cds.cern.ch/record/597182engMerlo, J PDumanoglu, IAkchurin, NAkgun, UAyan, SBrücken, PEskut, EFenyvesi, AKayis-Topaksu, AKoca, NMakónyi, KNovák, DÖnel, Y MOnengüt, GPolatoz, ARadiation-hardness studies of high OH**- content quartz fibres irradiated with 500 MeV electronsDetectors and Experimental TechniquesWe investigated the darkening of nine high OH**- fibre types irradiated with 500 MeV electrons from the Linac Injector of LEP (LIL) at CERN. The transmission of Xe light was measured in situ in the 350-800 nm range. The induced attenuation at 450 nm is typically 1.52 plus or minus 0.15 dB/m for a 100 Mrad absorbed dose. Two- parameter fits for darkening and recovery are presented. After irradiation the tensile strength remains essentially unchanged. For Polymicro quartz core fibres the tensile strength is typically 4.6 plus or minus 0.4 GPa.oai:cds.cern.ch:5971822002 |
spellingShingle | Detectors and Experimental Techniques Merlo, J P Dumanoglu, I Akchurin, N Akgun, U Ayan, S Brücken, P Eskut, E Fenyvesi, A Kayis-Topaksu, A Koca, N Makónyi, K Novák, D Önel, Y M Onengüt, G Polatoz, A Radiation-hardness studies of high OH**- content quartz fibres irradiated with 500 MeV electrons |
title | Radiation-hardness studies of high OH**- content quartz fibres irradiated with 500 MeV electrons |
title_full | Radiation-hardness studies of high OH**- content quartz fibres irradiated with 500 MeV electrons |
title_fullStr | Radiation-hardness studies of high OH**- content quartz fibres irradiated with 500 MeV electrons |
title_full_unstemmed | Radiation-hardness studies of high OH**- content quartz fibres irradiated with 500 MeV electrons |
title_short | Radiation-hardness studies of high OH**- content quartz fibres irradiated with 500 MeV electrons |
title_sort | radiation-hardness studies of high oh**- content quartz fibres irradiated with 500 mev electrons |
topic | Detectors and Experimental Techniques |
url | https://dx.doi.org/10.1016/S0168-9002(02)01067-7 http://cds.cern.ch/record/597182 |
work_keys_str_mv | AT merlojp radiationhardnessstudiesofhighohcontentquartzfibresirradiatedwith500mevelectrons AT dumanoglui radiationhardnessstudiesofhighohcontentquartzfibresirradiatedwith500mevelectrons AT akchurinn radiationhardnessstudiesofhighohcontentquartzfibresirradiatedwith500mevelectrons AT akgunu radiationhardnessstudiesofhighohcontentquartzfibresirradiatedwith500mevelectrons AT ayans radiationhardnessstudiesofhighohcontentquartzfibresirradiatedwith500mevelectrons AT bruckenp radiationhardnessstudiesofhighohcontentquartzfibresirradiatedwith500mevelectrons AT eskute radiationhardnessstudiesofhighohcontentquartzfibresirradiatedwith500mevelectrons AT fenyvesia radiationhardnessstudiesofhighohcontentquartzfibresirradiatedwith500mevelectrons AT kayistopaksua radiationhardnessstudiesofhighohcontentquartzfibresirradiatedwith500mevelectrons AT kocan radiationhardnessstudiesofhighohcontentquartzfibresirradiatedwith500mevelectrons AT makonyik radiationhardnessstudiesofhighohcontentquartzfibresirradiatedwith500mevelectrons AT novakd radiationhardnessstudiesofhighohcontentquartzfibresirradiatedwith500mevelectrons AT onelym radiationhardnessstudiesofhighohcontentquartzfibresirradiatedwith500mevelectrons AT onengutg radiationhardnessstudiesofhighohcontentquartzfibresirradiatedwith500mevelectrons AT polatoza radiationhardnessstudiesofhighohcontentquartzfibresirradiatedwith500mevelectrons |