Development of a Uniformisation Procedure for the PbW04 Crystals of the CMS Electromagnetic Calorimeter
The CMS electromagnetic calorimeter will consist of nearly 80,000 lead tungstate crystals, with 18 different geometries. The contribution of any non-uniformity in the light collection to the constant term in the energy resolution must be limited to 0.3%. A procedure capable of achieving this for the...
Autores principales: | , , , , , , |
---|---|
Lenguaje: | eng |
Publicado: |
2001
|
Materias: | |
Acceso en línea: | http://cds.cern.ch/record/687310 |
_version_ | 1780901730887663616 |
---|---|
author | Auffray, Etiennette Davies, Gavin Lebeau, Michel Lecoq, Paul Paoletti, Simone Schneegans, Marc Sempere-Roldan, P |
author_facet | Auffray, Etiennette Davies, Gavin Lebeau, Michel Lecoq, Paul Paoletti, Simone Schneegans, Marc Sempere-Roldan, P |
author_sort | Auffray, Etiennette |
collection | CERN |
description | The CMS electromagnetic calorimeter will consist of nearly 80,000 lead tungstate crystals, with 18 different geometries. The contribution of any non-uniformity in the light collection to the constant term in the energy resolution must be limited to 0.3%. A procedure capable of achieving this for the full calorimeter has been developed in the CERN EP-CMA group. A description of this method and the results obtained with the first few hundred pre-production crystals from Bogoroditsk, Russia are given in this note. |
id | cern-687310 |
institution | Organización Europea para la Investigación Nuclear |
language | eng |
publishDate | 2001 |
record_format | invenio |
spelling | cern-6873102019-09-30T06:29:59Zhttp://cds.cern.ch/record/687310engAuffray, EtiennetteDavies, GavinLebeau, MichelLecoq, PaulPaoletti, SimoneSchneegans, MarcSempere-Roldan, PDevelopment of a Uniformisation Procedure for the PbW04 Crystals of the CMS Electromagnetic CalorimeterDetectors and Experimental TechniquesThe CMS electromagnetic calorimeter will consist of nearly 80,000 lead tungstate crystals, with 18 different geometries. The contribution of any non-uniformity in the light collection to the constant term in the energy resolution must be limited to 0.3%. A procedure capable of achieving this for the full calorimeter has been developed in the CERN EP-CMA group. A description of this method and the results obtained with the first few hundred pre-production crystals from Bogoroditsk, Russia are given in this note.CMS-NOTE-2001-004oai:cds.cern.ch:6873102001-01-18 |
spellingShingle | Detectors and Experimental Techniques Auffray, Etiennette Davies, Gavin Lebeau, Michel Lecoq, Paul Paoletti, Simone Schneegans, Marc Sempere-Roldan, P Development of a Uniformisation Procedure for the PbW04 Crystals of the CMS Electromagnetic Calorimeter |
title | Development of a Uniformisation Procedure for the PbW04 Crystals of the CMS Electromagnetic Calorimeter |
title_full | Development of a Uniformisation Procedure for the PbW04 Crystals of the CMS Electromagnetic Calorimeter |
title_fullStr | Development of a Uniformisation Procedure for the PbW04 Crystals of the CMS Electromagnetic Calorimeter |
title_full_unstemmed | Development of a Uniformisation Procedure for the PbW04 Crystals of the CMS Electromagnetic Calorimeter |
title_short | Development of a Uniformisation Procedure for the PbW04 Crystals of the CMS Electromagnetic Calorimeter |
title_sort | development of a uniformisation procedure for the pbw04 crystals of the cms electromagnetic calorimeter |
topic | Detectors and Experimental Techniques |
url | http://cds.cern.ch/record/687310 |
work_keys_str_mv | AT auffrayetiennette developmentofauniformisationprocedureforthepbw04crystalsofthecmselectromagneticcalorimeter AT daviesgavin developmentofauniformisationprocedureforthepbw04crystalsofthecmselectromagneticcalorimeter AT lebeaumichel developmentofauniformisationprocedureforthepbw04crystalsofthecmselectromagneticcalorimeter AT lecoqpaul developmentofauniformisationprocedureforthepbw04crystalsofthecmselectromagneticcalorimeter AT paolettisimone developmentofauniformisationprocedureforthepbw04crystalsofthecmselectromagneticcalorimeter AT schneegansmarc developmentofauniformisationprocedureforthepbw04crystalsofthecmselectromagneticcalorimeter AT sempereroldanp developmentofauniformisationprocedureforthepbw04crystalsofthecmselectromagneticcalorimeter |