First results on radiation damage in PbWO4 crystals exposed to a 20 GeV/c proton beam
We have exposed seven full length production quality crystals of the electromagnetic calorimeter (ECAL) of the CMS detector to a 20 GeV/c proton beam at the CERN PS accelerator. The exposure was done at fluxes of 10**12 p/cm**2/h and 10**13 p/cm**2/h and integral fluences of 10**12 p/cm**2 and 10**1...
Autores principales: | , , , |
---|---|
Lenguaje: | eng |
Publicado: |
2003
|
Materias: | |
Acceso en línea: | https://dx.doi.org/10.1142/9789812702708_0096 http://cds.cern.ch/record/691154 |
Sumario: | We have exposed seven full length production quality crystals of the electromagnetic calorimeter (ECAL) of the CMS detector to a 20 GeV/c proton beam at the CERN PS accelerator. The exposure was done at fluxes of 10**12 p/cm**2/h and 10**13 p/cm**2/h and integral fluences of 10**12 p/cm**2 and 10**13 p/cm**2 were reached at both rates. The light transmission of the crystals was measured after irradiation and suitable cooling time for induced radioactivity to decrease to a safe level. First results of these measurements are shown. The possible damage mechanisms are discussed and simulations based on one possible model are presented. The implications for long-term operation of CMS are discussed and it is shown that in the whole barrel and at least most of the ECAL endcap hadron damage alone - even if cumulative - should not cause the crystals to fail the CMS specification of an induced absorption coefficient muIND < 1.5 /m during the first 10 years of LHC operation. |
---|