Fatigue Testing of Materials by UV Pulsed Laser Irradiation
The energy dissipated by the RF currents in the cavities of pulsed high-power linacs induces cycles of the surface temperature. In the case of the CLIC main linac the expected amplitude of the thermal cycles is above fifty degrees, for a total number of pulses reaching 1011. The differential thermal...
Autores principales: | Calatroni, S, Neupert, H, Taborelli, M |
---|---|
Lenguaje: | eng |
Publicado: |
2004
|
Materias: | |
Acceso en línea: | http://cds.cern.ch/record/801190 |
Ejemplares similares
-
Evolution of surface topography in dependence on the grain orientation during surface thermal fatigue of polycrystalline copper
por: Aicheler, M, et al.
Publicado: (2011) -
Breakdown resistance of refractory metals compared to copper
por: Taborelli, M, et al.
Publicado: (2004) -
DC Breakdown experiments for CLIC
por: Descoeudres, A, et al.
Publicado: (2008) -
Fatigue of materials
por: Suresh, Subra
Publicado: (1998) -
A short summary of the R&D activity carried out at CERN in the past five years and ideas for further R&D based on the present state of the art
por: Calatroni, Sergio, et al.
Publicado: (2000)