Mapping residual stresses in PbWO$_{4}$ crystals using photo-elastic analysis
Large scintillating crystals are affected by internal stresses induced by the crystal growth temperature gradient remanence. Cutting boules (ingots) into finished crystal shapes allows for a partial tension relaxation but residual stresses remain the main cause of breaking. Quality control of residu...
Autores principales: | Lebeau, Michel, Gobbi, L, Majni, G, Paone, N, Pietroni, P, Rinaldi, D |
---|---|
Lenguaje: | eng |
Publicado: |
2005
|
Materias: | |
Acceso en línea: | https://dx.doi.org/10.1016/j.nima.2004.07.256 http://cds.cern.ch/record/912958 |
Ejemplares similares
-
Surface quality inspection of PbWO$_{4}$ crystals by grazing incidence X-ray diffraction
por: Mengucci, P, et al.
Publicado: (2005) -
Quality control on pre-serial Bridgman production of PbWO(4) scintillating crystals by means of photoelasticity
por: Rinaldi, D, et al.
Publicado: (2010) -
PWO photo-elastic parameter calibration by laser-based polariscope
por: Ciriaco, A, et al.
Publicado: (2007) -
Light collection in $PbWO_{4}$ crystals
por: Paoletti, S, et al.
Publicado: (1999) -
Photoelasticimetry for the inspection of mechanical stresses in birefringent monoaxial crystals: application to $PbWO_{4}$
por: Lebeau, M, et al.
Publicado: (1997)