Effect of a Nickel Coating Applied on the Inner Wall of the BPM Supports of LHC
All of the special BPMs, e.g., used for tune and chromaticity measurements in LHC Point 4 will be treated such as to have the standard copper layer on the inside of the beam pipe. Between the stainless steel pipe and the copper layer, a 1 µm nickel coating will be applied. This nickel layer might c...
Autor principal: | |
---|---|
Lenguaje: | eng |
Publicado: |
2006
|
Materias: | |
Acceso en línea: | http://cds.cern.ch/record/950800 |
_version_ | 1780909965353943040 |
---|---|
author | Völlinger, C |
author_facet | Völlinger, C |
author_sort | Völlinger, C |
collection | CERN |
description | All of the special BPMs, e.g., used for tune and chromaticity measurements in LHC Point 4 will be treated such as to have the standard copper layer on the inside of the beam pipe. Between the stainless steel pipe and the copper layer, a 1 µm nickel coating will be applied. This nickel layer might cause a problem if an electrolytic process is used for the plating which could cause a permanent magnetization of the layer similarly as it was observed for LEP. This note gives an estimation of the effect to be expected. |
id | cern-950800 |
institution | Organización Europea para la Investigación Nuclear |
language | eng |
publishDate | 2006 |
record_format | invenio |
spelling | cern-9508002019-09-30T06:29:59Zhttp://cds.cern.ch/record/950800engVöllinger, CEffect of a Nickel Coating Applied on the Inner Wall of the BPM Supports of LHCAccelerators and Storage RingsAll of the special BPMs, e.g., used for tune and chromaticity measurements in LHC Point 4 will be treated such as to have the standard copper layer on the inside of the beam pipe. Between the stainless steel pipe and the copper layer, a 1 µm nickel coating will be applied. This nickel layer might cause a problem if an electrolytic process is used for the plating which could cause a permanent magnetization of the layer similarly as it was observed for LEP. This note gives an estimation of the effect to be expected.LHC-Project-Note-384CERN-LHC-Project-Note-384oai:cds.cern.ch:9508002006-05-16 |
spellingShingle | Accelerators and Storage Rings Völlinger, C Effect of a Nickel Coating Applied on the Inner Wall of the BPM Supports of LHC |
title | Effect of a Nickel Coating Applied on the Inner Wall of the BPM Supports of LHC |
title_full | Effect of a Nickel Coating Applied on the Inner Wall of the BPM Supports of LHC |
title_fullStr | Effect of a Nickel Coating Applied on the Inner Wall of the BPM Supports of LHC |
title_full_unstemmed | Effect of a Nickel Coating Applied on the Inner Wall of the BPM Supports of LHC |
title_short | Effect of a Nickel Coating Applied on the Inner Wall of the BPM Supports of LHC |
title_sort | effect of a nickel coating applied on the inner wall of the bpm supports of lhc |
topic | Accelerators and Storage Rings |
url | http://cds.cern.ch/record/950800 |
work_keys_str_mv | AT vollingerc effectofanickelcoatingappliedontheinnerwallofthebpmsupportsoflhc |