Cargando…

Evidence for length-dependent wire expansion, filament dedensification and consequent degradation of critical current density in Ag-alloy sheathed Bi-2212 wires

It is well known that longer Bi-2212 conductors have significantly lower critical current density (Jc) than shorter ones, and recently it has become clear that a major cause of this reduction is internal gas pressure generated during heat treatment, which expands the wire diameter and dedensifies th...

Descripción completa

Detalles Bibliográficos
Autores principales: Malagoli, A, Lee, P J, Ghosh, A K, Scheuerlein, C, Di Michiel, M, Jiang, J, Trociewitz, U P, Hellstrom, E E, Larbalestier, D C