Cargando…
Measurement of NEG Coating Performance Variation in the LHC after the First Long Shutdown
During the Long Shutdown 1 (LS1) of the Large Hadron Collider, 90% of the Non-Evaporable Getter (NEG) coated beam pipes in the Long Straight Sections (LSS) were vented to undertake the planned upgrade and consolidation programmes. After each intervention, an additional bake-out and NEG activation we...
Autores principales: | , , , , , |
---|---|
Lenguaje: | eng |
Publicado: |
2015
|
Materias: | |
Acceso en línea: | http://cds.cern.ch/record/2141870 |
Sumario: | During the Long Shutdown 1 (LS1) of the Large Hadron Collider, 90% of the Non-Evaporable Getter (NEG) coated beam pipes in the Long Straight Sections (LSS) were vented to undertake the planned upgrade and consolidation programmes. After each intervention, an additional bake-out and NEG activation were performed to reach the vacuum requirements. An analysis of the coating performance variation after the additional activation cycle has been carried out by using ultimate pressure and pressure build-up measurements. In addition, laboratory measurements have been carried out to mimic the LHC coated beam pipe behaviour. The experimental data have been compared with calculation obtained by Molflow+. |
---|