Fatigue performance evaluation for ITER IVC conductor component materials

The ITER IVCs are made of stainless steel mineral-insulated conductors composed by an OFE copper conductor and a SS316LN jacket. The baseline design requires the coils to endure all ITER machine life time. After a brief review of past and recent literatures, no results are available and of our inter...

Descripción completa

Detalles Bibliográficos
Autores principales: Jin, H, Vostner, A, Wu, Y, Macioce, D, Sgobba, S, Huang, C, Romero Rodriguez, C, Fernandez Pison, P, Elisabeth Langeslag, S A, Aviles Santillana, I, Long, F, Yu, M, Tao, B
Lenguaje:eng
Publicado: 2017
Materias:
Acceso en línea:https://dx.doi.org/10.1016/j.vacuum.2017.08.023
http://cds.cern.ch/record/2318244
_version_ 1780958448329949184
author Jin, H
Vostner, A
Wu, Y
Macioce, D
Sgobba, S
Huang, C
Romero Rodriguez, C
Fernandez Pison, P
Elisabeth Langeslag, S A
Aviles Santillana, I
Long, F
Yu, M
Tao, B
author_facet Jin, H
Vostner, A
Wu, Y
Macioce, D
Sgobba, S
Huang, C
Romero Rodriguez, C
Fernandez Pison, P
Elisabeth Langeslag, S A
Aviles Santillana, I
Long, F
Yu, M
Tao, B
author_sort Jin, H
collection CERN
description The ITER IVCs are made of stainless steel mineral-insulated conductors composed by an OFE copper conductor and a SS316LN jacket. The baseline design requires the coils to endure all ITER machine life time. After a brief review of past and recent literatures, no results are available and of our interest. Moreover, cold working, aging treatments as well as the environment temperature affect the mechanical and fatigue properties. The present paper summarizes data from tensile and uniaxial tension load controlled fatigue tests on both the steel jacket and the copper conductor in the IVC representative operation conditions. Tests are performed on specimens sectioned from the tubes undergone cold working of conductor compaction, coil winding and so on as well as heat treatment at 240 °C for 24 h of baking, and finally tested at operation temperature of 120 °C. The fatigue tests were conducted at frequency of 15 Hz and the stress ratio of R = 0.1. Results from tensile tests show both strength and ductility decrease as temperature rises from RT to 120 °C. Results from fatigue tests are presented as S-N relationships with the maximum stress expressed as a percentage of the strength under static loading. It was found that the fatigue strength limit for OFE copper conductor and SS316LN jacket were close to 120 MPa and 275 MPa respectively. The influence from residual stresses on the static and fatigue performance of 316LN jacket were also investigated It was found that the ductility and fatigue life can be improved by residual stress releasing of heat treatment at 650 °C for 100 h.
id oai-inspirehep.net-1667132
institution Organización Europea para la Investigación Nuclear
language eng
publishDate 2017
record_format invenio
spelling oai-inspirehep.net-16671322019-09-30T06:29:59Zdoi:10.1016/j.vacuum.2017.08.023http://cds.cern.ch/record/2318244engJin, HVostner, AWu, YMacioce, DSgobba, SHuang, CRomero Rodriguez, CFernandez Pison, PElisabeth Langeslag, S AAviles Santillana, ILong, FYu, MTao, BFatigue performance evaluation for ITER IVC conductor component materialsDetectors and Experimental TechniquesThe ITER IVCs are made of stainless steel mineral-insulated conductors composed by an OFE copper conductor and a SS316LN jacket. The baseline design requires the coils to endure all ITER machine life time. After a brief review of past and recent literatures, no results are available and of our interest. Moreover, cold working, aging treatments as well as the environment temperature affect the mechanical and fatigue properties. The present paper summarizes data from tensile and uniaxial tension load controlled fatigue tests on both the steel jacket and the copper conductor in the IVC representative operation conditions. Tests are performed on specimens sectioned from the tubes undergone cold working of conductor compaction, coil winding and so on as well as heat treatment at 240 °C for 24 h of baking, and finally tested at operation temperature of 120 °C. The fatigue tests were conducted at frequency of 15 Hz and the stress ratio of R = 0.1. Results from tensile tests show both strength and ductility decrease as temperature rises from RT to 120 °C. Results from fatigue tests are presented as S-N relationships with the maximum stress expressed as a percentage of the strength under static loading. It was found that the fatigue strength limit for OFE copper conductor and SS316LN jacket were close to 120 MPa and 275 MPa respectively. The influence from residual stresses on the static and fatigue performance of 316LN jacket were also investigated It was found that the ductility and fatigue life can be improved by residual stress releasing of heat treatment at 650 °C for 100 h.oai:inspirehep.net:16671322017
spellingShingle Detectors and Experimental Techniques
Jin, H
Vostner, A
Wu, Y
Macioce, D
Sgobba, S
Huang, C
Romero Rodriguez, C
Fernandez Pison, P
Elisabeth Langeslag, S A
Aviles Santillana, I
Long, F
Yu, M
Tao, B
Fatigue performance evaluation for ITER IVC conductor component materials
title Fatigue performance evaluation for ITER IVC conductor component materials
title_full Fatigue performance evaluation for ITER IVC conductor component materials
title_fullStr Fatigue performance evaluation for ITER IVC conductor component materials
title_full_unstemmed Fatigue performance evaluation for ITER IVC conductor component materials
title_short Fatigue performance evaluation for ITER IVC conductor component materials
title_sort fatigue performance evaluation for iter ivc conductor component materials
topic Detectors and Experimental Techniques
url https://dx.doi.org/10.1016/j.vacuum.2017.08.023
http://cds.cern.ch/record/2318244
work_keys_str_mv AT jinh fatigueperformanceevaluationforiterivcconductorcomponentmaterials
AT vostnera fatigueperformanceevaluationforiterivcconductorcomponentmaterials
AT wuy fatigueperformanceevaluationforiterivcconductorcomponentmaterials
AT macioced fatigueperformanceevaluationforiterivcconductorcomponentmaterials
AT sgobbas fatigueperformanceevaluationforiterivcconductorcomponentmaterials
AT huangc fatigueperformanceevaluationforiterivcconductorcomponentmaterials
AT romerorodriguezc fatigueperformanceevaluationforiterivcconductorcomponentmaterials
AT fernandezpisonp fatigueperformanceevaluationforiterivcconductorcomponentmaterials
AT elisabethlangeslagsa fatigueperformanceevaluationforiterivcconductorcomponentmaterials
AT avilessantillanai fatigueperformanceevaluationforiterivcconductorcomponentmaterials
AT longf fatigueperformanceevaluationforiterivcconductorcomponentmaterials
AT yum fatigueperformanceevaluationforiterivcconductorcomponentmaterials
AT taob fatigueperformanceevaluationforiterivcconductorcomponentmaterials