Effect of Denture Disinfectants on the Mechanical Performance of 3D-Printed Denture Base Materials

Denture care and maintenance are necessary for both denture longevity and underlying tissue health. However, the effects of disinfectants on the strength of 3D-printed denture base resins are unclear. Herein, distilled water (DW), effervescent tablet, and sodium hypochlorite (NaOCl) immersion soluti...

Descripción completa

Detalles Bibliográficos
Autores principales: Alkaltham, Nora S., Aldhafiri, Reem A., Al-Thobity, Ahmad M., Alramadan, Hassan, Aljubran, Hussain, Ateeq, Ijlal Shahrukh, Khan, Soban Q., Akhtar, Sultan, Gad, Mohammed M.
Formato: Online Artículo Texto
Lenguaje:English
Publicado: MDPI 2023
Materias:
Acceso en línea:https://www.ncbi.nlm.nih.gov/pmc/articles/PMC10007094/
https://www.ncbi.nlm.nih.gov/pubmed/36904416
http://dx.doi.org/10.3390/polym15051175
Descripción
Sumario:Denture care and maintenance are necessary for both denture longevity and underlying tissue health. However, the effects of disinfectants on the strength of 3D-printed denture base resins are unclear. Herein, distilled water (DW), effervescent tablet, and sodium hypochlorite (NaOCl) immersion solutions were used to investigate the flexural properties and hardness of two 3D-printed resins (NextDent and FormLabs) compared with a heat-polymerized resin. The flexural strength and elastic modulus were investigated using the three-point bending test and Vickers hardness test before (baseline) immersion and 180 days after immersion. The data were analyzed using ANOVA and Tukey’s post hoc test (α = 0.05), and further verified by using electron microscopy and infrared spectroscopy. The flexural strength of all the materials decreased after solution immersion (p < 0.001). The effervescent tablet and NaOCl immersion reduced the flexural strength (p < 0.001), with the lowest values recorded with the NaOCl immersion. The elastic modulus did not significantly differ between the baseline and after the DW immersion (p > 0.05), but significantly decreased after the effervescent tablet and NaOCl immersion (p < 0.001). The hardness significantly decreased after immersion in all the solutions (p < 0.001). The immersion of the heat-polymerized and 3D-printed resins in the DW and disinfectant solutions decreased the flexural properties and hardness.