Cargando…
Antibacterial activity and shear bond strength of fiber-reinforced composites and bonding agents containing 0.5%, 1%, 2.5%, and 5% silver nanoparticles
BACKGROUND: Bonded composites may increase bacterial accumulation and caries formation risk. Therefore, assessment of methods to decrease bacterial activity around them would be valuable. The literature on the efficacy of adding silver nanoparticles to fiber-reinforced composite (FRC) or adding them...
Autores principales: | , , , , |
---|---|
Formato: | Online Artículo Texto |
Lenguaje: | English |
Publicado: |
Wolters Kluwer - Medknow
2023
|
Materias: | |
Acceso en línea: | https://www.ncbi.nlm.nih.gov/pmc/articles/PMC10028584/ https://www.ncbi.nlm.nih.gov/pubmed/36960016 http://dx.doi.org/10.4103/1735-3327.369625 |
_version_ | 1784909978019037184 |
---|---|
author | Jenabi, Nastaran Sadeghian, Susan Karimzadeh, Fathallah Pour, Maryam Safavi Rakhshan, Vahid |
author_facet | Jenabi, Nastaran Sadeghian, Susan Karimzadeh, Fathallah Pour, Maryam Safavi Rakhshan, Vahid |
author_sort | Jenabi, Nastaran |
collection | PubMed |
description | BACKGROUND: Bonded composites may increase bacterial accumulation and caries formation risk. Therefore, assessment of methods to decrease bacterial activity around them would be valuable. The literature on the efficacy of adding silver nanoparticles to fiber-reinforced composite (FRC) or adding them to bonding agents in terms of their antibacterial activity and/or shear bond strength (SBS) is scarce. Thus, we aimed to assess the antibacterial activity of flowable composites and bonding agents containing various percentages of experimental silver nanoparticles (nanosilver) against S. mutans and to evaluate the SBS of FRC and bonding agents containing different amounts of nanosilver to enamel. MATERIALS AND METHODS: In this preliminary study, 0% (control), 0.5%, 1%, 2.5%, and 5% nanosilver were added to flowable composite and bonding agent. Syntheses of nanosilver and nanosilver-incorporated composite specimens were approved using X-ray diffraction spectroscopy and scanning electron microscopy. Antibacterial effects of the produced materials on S. mutans were evaluated by colony count with serial dilution method (n = 7 groups × 10 [n = 70] specimens) and agar disc diffusion test (n = 6 groups × 5 [n = 30] composite specimens + n = 6 groups × 5 [n = 30] light-cured bonding + n = 6 groups × 5 [n = 30] uncured bonding) against negative control and cefotaxime antibiotic. Moreover, SBS values of various FRC blocks bonded to enamel using various bonding agents were measured (n = 9 groups × 6 [n = 54] human premolars). Data were analyzed using Kruskal–Wallis, Dunn, two-way analysis of variance, and Tukey's tests (α = 0.05). RESULTS: Composite discs containing all concentrations of nanosilver reduced S. mutans colony counts (P < 0.05); bacterial growth was ceased at samples containing 2.5% and 5% of nanosilver. The reduction in the SBS of FRCs was significant only for 5% nanosilver (P < 0.05). CONCLUSION: Adding 0.5%, 1%, and 2.5% nanosilver to composite and 0.5% or 1% nanosilver to bonding agent led to a significant antibacterial behavior against S. mutans while not significantly affecting the SBS of FRC. |
format | Online Article Text |
id | pubmed-10028584 |
institution | National Center for Biotechnology Information |
language | English |
publishDate | 2023 |
publisher | Wolters Kluwer - Medknow |
record_format | MEDLINE/PubMed |
spelling | pubmed-100285842023-03-22 Antibacterial activity and shear bond strength of fiber-reinforced composites and bonding agents containing 0.5%, 1%, 2.5%, and 5% silver nanoparticles Jenabi, Nastaran Sadeghian, Susan Karimzadeh, Fathallah Pour, Maryam Safavi Rakhshan, Vahid Dent Res J (Isfahan) Original Article BACKGROUND: Bonded composites may increase bacterial accumulation and caries formation risk. Therefore, assessment of methods to decrease bacterial activity around them would be valuable. The literature on the efficacy of adding silver nanoparticles to fiber-reinforced composite (FRC) or adding them to bonding agents in terms of their antibacterial activity and/or shear bond strength (SBS) is scarce. Thus, we aimed to assess the antibacterial activity of flowable composites and bonding agents containing various percentages of experimental silver nanoparticles (nanosilver) against S. mutans and to evaluate the SBS of FRC and bonding agents containing different amounts of nanosilver to enamel. MATERIALS AND METHODS: In this preliminary study, 0% (control), 0.5%, 1%, 2.5%, and 5% nanosilver were added to flowable composite and bonding agent. Syntheses of nanosilver and nanosilver-incorporated composite specimens were approved using X-ray diffraction spectroscopy and scanning electron microscopy. Antibacterial effects of the produced materials on S. mutans were evaluated by colony count with serial dilution method (n = 7 groups × 10 [n = 70] specimens) and agar disc diffusion test (n = 6 groups × 5 [n = 30] composite specimens + n = 6 groups × 5 [n = 30] light-cured bonding + n = 6 groups × 5 [n = 30] uncured bonding) against negative control and cefotaxime antibiotic. Moreover, SBS values of various FRC blocks bonded to enamel using various bonding agents were measured (n = 9 groups × 6 [n = 54] human premolars). Data were analyzed using Kruskal–Wallis, Dunn, two-way analysis of variance, and Tukey's tests (α = 0.05). RESULTS: Composite discs containing all concentrations of nanosilver reduced S. mutans colony counts (P < 0.05); bacterial growth was ceased at samples containing 2.5% and 5% of nanosilver. The reduction in the SBS of FRCs was significant only for 5% nanosilver (P < 0.05). CONCLUSION: Adding 0.5%, 1%, and 2.5% nanosilver to composite and 0.5% or 1% nanosilver to bonding agent led to a significant antibacterial behavior against S. mutans while not significantly affecting the SBS of FRC. Wolters Kluwer - Medknow 2023-02-14 /pmc/articles/PMC10028584/ /pubmed/36960016 http://dx.doi.org/10.4103/1735-3327.369625 Text en Copyright: © 2023 Dental Research Journal https://creativecommons.org/licenses/by-nc-sa/4.0/This is an open access journal, and articles are distributed under the terms of the Creative Commons Attribution-NonCommercial-ShareAlike 4.0 License, which allows others to remix, tweak, and build upon the work non-commercially, as long as appropriate credit is given and the new creations are licensed under the identical terms. |
spellingShingle | Original Article Jenabi, Nastaran Sadeghian, Susan Karimzadeh, Fathallah Pour, Maryam Safavi Rakhshan, Vahid Antibacterial activity and shear bond strength of fiber-reinforced composites and bonding agents containing 0.5%, 1%, 2.5%, and 5% silver nanoparticles |
title | Antibacterial activity and shear bond strength of fiber-reinforced composites and bonding agents containing 0.5%, 1%, 2.5%, and 5% silver nanoparticles |
title_full | Antibacterial activity and shear bond strength of fiber-reinforced composites and bonding agents containing 0.5%, 1%, 2.5%, and 5% silver nanoparticles |
title_fullStr | Antibacterial activity and shear bond strength of fiber-reinforced composites and bonding agents containing 0.5%, 1%, 2.5%, and 5% silver nanoparticles |
title_full_unstemmed | Antibacterial activity and shear bond strength of fiber-reinforced composites and bonding agents containing 0.5%, 1%, 2.5%, and 5% silver nanoparticles |
title_short | Antibacterial activity and shear bond strength of fiber-reinforced composites and bonding agents containing 0.5%, 1%, 2.5%, and 5% silver nanoparticles |
title_sort | antibacterial activity and shear bond strength of fiber-reinforced composites and bonding agents containing 0.5%, 1%, 2.5%, and 5% silver nanoparticles |
topic | Original Article |
url | https://www.ncbi.nlm.nih.gov/pmc/articles/PMC10028584/ https://www.ncbi.nlm.nih.gov/pubmed/36960016 http://dx.doi.org/10.4103/1735-3327.369625 |
work_keys_str_mv | AT jenabinastaran antibacterialactivityandshearbondstrengthoffiberreinforcedcompositesandbondingagentscontaining05125and5silvernanoparticles AT sadeghiansusan antibacterialactivityandshearbondstrengthoffiberreinforcedcompositesandbondingagentscontaining05125and5silvernanoparticles AT karimzadehfathallah antibacterialactivityandshearbondstrengthoffiberreinforcedcompositesandbondingagentscontaining05125and5silvernanoparticles AT pourmaryamsafavi antibacterialactivityandshearbondstrengthoffiberreinforcedcompositesandbondingagentscontaining05125and5silvernanoparticles AT rakhshanvahid antibacterialactivityandshearbondstrengthoffiberreinforcedcompositesandbondingagentscontaining05125and5silvernanoparticles |