Cargando…

Effect of Anti-COVID-19 Mouthwashes on Shear Bond Strength of Resin-Matrix Ceramics Repaired with Resin Composite Using Universal Adhesive: An In Vitro Study

Using anti-COVID-19 mouthwashes has become necessary to reduce acute respiratory syndrome coronavirus 2 (SARS-CoV-2) transmissions. Resin-matrix ceramic (RMCs) materials that are exposed to mouthwashes may affect the bonding of repaired materials. This research was performed to assess the effects of...

Descripción completa

Detalles Bibliográficos
Autores principales: Limsiriwong, Wichuda, Klaisiri, Awiruth, Krajangta, Nantawan
Formato: Online Artículo Texto
Lenguaje:English
Publicado: MDPI 2023
Materias:
Acceso en línea:https://www.ncbi.nlm.nih.gov/pmc/articles/PMC10052296/
https://www.ncbi.nlm.nih.gov/pubmed/36976082
http://dx.doi.org/10.3390/jfb14030158
_version_ 1785015127419912192
author Limsiriwong, Wichuda
Klaisiri, Awiruth
Krajangta, Nantawan
author_facet Limsiriwong, Wichuda
Klaisiri, Awiruth
Krajangta, Nantawan
author_sort Limsiriwong, Wichuda
collection PubMed
description Using anti-COVID-19 mouthwashes has become necessary to reduce acute respiratory syndrome coronavirus 2 (SARS-CoV-2) transmissions. Resin-matrix ceramic (RMCs) materials that are exposed to mouthwashes may affect the bonding of repaired materials. This research was performed to assess the effects of anti-COVID-19 mouthwashes on the shear bond strengths (SBS) of RMCs repaired with resin composites. A total of 189 rectangular specimens of two different RMCs (Vita Enamic (VE) and Shofu Block HC (ShB)) were thermocycled and randomly divided into nine subgroups according to different mouthwashes (distilled water (DW), 0.2% povidone–iodine (PVP-I), and 1.5% hydrogen peroxide (HP)) and surface treatment protocols (no surface treatment, hydrofluoric acid etching (HF), and sandblasting (SB)). A repair protocol for RMCs was performed (using universal adhesives and resin composites), and the specimens were assessed using an SBS test. The failure mode was examined using a stereomicroscope. The SBS data were evaluated using a three-way ANOVA and a Tukey post hoc test. The SBS were significantly affected by the RMCs, mouthwashes, and surface treatment protocols. Both surface treatment protocols (HF and SB) for both RMCs, whether immersed in anti-COVID-19 mouthwash or not, improved the SBS. For the VE immersed in HP and PVP-I, the HF surface treatment had the highest SBS. For the ShB immersed in HP and PVP-I, the SB surface treatment had the highest SBS.
format Online
Article
Text
id pubmed-10052296
institution National Center for Biotechnology Information
language English
publishDate 2023
publisher MDPI
record_format MEDLINE/PubMed
spelling pubmed-100522962023-03-30 Effect of Anti-COVID-19 Mouthwashes on Shear Bond Strength of Resin-Matrix Ceramics Repaired with Resin Composite Using Universal Adhesive: An In Vitro Study Limsiriwong, Wichuda Klaisiri, Awiruth Krajangta, Nantawan J Funct Biomater Article Using anti-COVID-19 mouthwashes has become necessary to reduce acute respiratory syndrome coronavirus 2 (SARS-CoV-2) transmissions. Resin-matrix ceramic (RMCs) materials that are exposed to mouthwashes may affect the bonding of repaired materials. This research was performed to assess the effects of anti-COVID-19 mouthwashes on the shear bond strengths (SBS) of RMCs repaired with resin composites. A total of 189 rectangular specimens of two different RMCs (Vita Enamic (VE) and Shofu Block HC (ShB)) were thermocycled and randomly divided into nine subgroups according to different mouthwashes (distilled water (DW), 0.2% povidone–iodine (PVP-I), and 1.5% hydrogen peroxide (HP)) and surface treatment protocols (no surface treatment, hydrofluoric acid etching (HF), and sandblasting (SB)). A repair protocol for RMCs was performed (using universal adhesives and resin composites), and the specimens were assessed using an SBS test. The failure mode was examined using a stereomicroscope. The SBS data were evaluated using a three-way ANOVA and a Tukey post hoc test. The SBS were significantly affected by the RMCs, mouthwashes, and surface treatment protocols. Both surface treatment protocols (HF and SB) for both RMCs, whether immersed in anti-COVID-19 mouthwash or not, improved the SBS. For the VE immersed in HP and PVP-I, the HF surface treatment had the highest SBS. For the ShB immersed in HP and PVP-I, the SB surface treatment had the highest SBS. MDPI 2023-03-16 /pmc/articles/PMC10052296/ /pubmed/36976082 http://dx.doi.org/10.3390/jfb14030158 Text en © 2023 by the authors. https://creativecommons.org/licenses/by/4.0/Licensee MDPI, Basel, Switzerland. This article is an open access article distributed under the terms and conditions of the Creative Commons Attribution (CC BY) license (https://creativecommons.org/licenses/by/4.0/).
spellingShingle Article
Limsiriwong, Wichuda
Klaisiri, Awiruth
Krajangta, Nantawan
Effect of Anti-COVID-19 Mouthwashes on Shear Bond Strength of Resin-Matrix Ceramics Repaired with Resin Composite Using Universal Adhesive: An In Vitro Study
title Effect of Anti-COVID-19 Mouthwashes on Shear Bond Strength of Resin-Matrix Ceramics Repaired with Resin Composite Using Universal Adhesive: An In Vitro Study
title_full Effect of Anti-COVID-19 Mouthwashes on Shear Bond Strength of Resin-Matrix Ceramics Repaired with Resin Composite Using Universal Adhesive: An In Vitro Study
title_fullStr Effect of Anti-COVID-19 Mouthwashes on Shear Bond Strength of Resin-Matrix Ceramics Repaired with Resin Composite Using Universal Adhesive: An In Vitro Study
title_full_unstemmed Effect of Anti-COVID-19 Mouthwashes on Shear Bond Strength of Resin-Matrix Ceramics Repaired with Resin Composite Using Universal Adhesive: An In Vitro Study
title_short Effect of Anti-COVID-19 Mouthwashes on Shear Bond Strength of Resin-Matrix Ceramics Repaired with Resin Composite Using Universal Adhesive: An In Vitro Study
title_sort effect of anti-covid-19 mouthwashes on shear bond strength of resin-matrix ceramics repaired with resin composite using universal adhesive: an in vitro study
topic Article
url https://www.ncbi.nlm.nih.gov/pmc/articles/PMC10052296/
https://www.ncbi.nlm.nih.gov/pubmed/36976082
http://dx.doi.org/10.3390/jfb14030158
work_keys_str_mv AT limsiriwongwichuda effectofanticovid19mouthwashesonshearbondstrengthofresinmatrixceramicsrepairedwithresincompositeusinguniversaladhesiveaninvitrostudy
AT klaisiriawiruth effectofanticovid19mouthwashesonshearbondstrengthofresinmatrixceramicsrepairedwithresincompositeusinguniversaladhesiveaninvitrostudy
AT krajangtanantawan effectofanticovid19mouthwashesonshearbondstrengthofresinmatrixceramicsrepairedwithresincompositeusinguniversaladhesiveaninvitrostudy