Effect of NO(2) Aging on the Surface Structure and Thermal Stability of Silicone Rubber with Varying Al(OH)(3) Contents
In this study, silicone rubber (SiR) with 0, 90, and 180 parts of aluminum hydroxide (Al(OH)(3), ATH) contents prepared in the laboratory was treated in a certain concentration of NO(2) for 0, 12, 24, and 36 h. Fourier transform-infrared spectroscopy (FT-IR), scanning electron microscopy (SEM), atom...
Autores principales: | Fang, Jiapeng, Luo, Yi, Kuang, Shilong, Luo, Kai, Xiao, Zikang, Peng, Xiangyang, Huang, Zhen, Wang, Zheng, Fang, Pengfei |
---|---|
Formato: | Online Artículo Texto |
Lenguaje: | English |
Publicado: |
MDPI
2023
|
Materias: | |
Acceso en línea: | https://www.ncbi.nlm.nih.gov/pmc/articles/PMC10054637/ https://www.ncbi.nlm.nih.gov/pubmed/36984420 http://dx.doi.org/10.3390/ma16062540 |
Ejemplares similares
-
The Influence of Titanium Dioxide Nanosheet on Water Permeability of Silicone Rubber after Nitrogen Dioxide Aging Treatment
por: Peng, Xiangyang, et al.
Publicado: (2023) -
Study on NO(2) Barrier Properties of RTV Silicone Rubber by Incorporation of Functional Graphene Oxide
por: Huang, Zhen, et al.
Publicado: (2023) -
Influence of Crosslinking Extent on Free Volumes of Silicone Rubber and Water Diffusion after Corona Discharge
por: Yang, Yue, et al.
Publicado: (2022) -
Synthesis of Zirconium-Containing Polyhedral Oligometallasilsesquioxane as an Efficient Thermal Stabilizer for Silicone Rubber
por: Qiu, Jiedong, et al.
Publicado: (2018) -
How the Crosslinking Agent Influences the Thermal Stability of RTV Phenyl Silicone Rubber
por: He, Chen, et al.
Publicado: (2018)