Cargando…

Microstructure Evolution and Mechanical Properties of Al–Cu–Mg Alloys with Si Addition

The aim of this study was to investigate the impact of the addition of a minor quantity of Si on the microstructure evolution, heat treatment response, and mechanical properties of the Al–4.5Cu–0.15Ti–3.0Mg alloy. The microstructure analysis of the base alloy revealed the presence of α-Al grains, eu...

Descripción completa

Detalles Bibliográficos
Autores principales: Shah, Abdul Wahid, Ha, Seong-Ho, Siddique, Jabir Ali, Kim, Bong-Hwan, Yoon, Young-Ok, Lim, Hyun-Kyu, Kim, Shae K.
Formato: Online Artículo Texto
Lenguaje:English
Publicado: MDPI 2023
Materias:
Acceso en línea:https://www.ncbi.nlm.nih.gov/pmc/articles/PMC10096403/
https://www.ncbi.nlm.nih.gov/pubmed/37049077
http://dx.doi.org/10.3390/ma16072783
Descripción
Sumario:The aim of this study was to investigate the impact of the addition of a minor quantity of Si on the microstructure evolution, heat treatment response, and mechanical properties of the Al–4.5Cu–0.15Ti–3.0Mg alloy. The microstructure analysis of the base alloy revealed the presence of α-Al grains, eutectic α-Al-Al(2)CuMg (S) phases, and Mg(32)(Al, Cu)(49) (T) phases within the Al grains. In contrast, the Si-added alloy featured the eutectic α-Al-Mg(2)Si phases, eutectic α-Al-S-Mg(2)Si, and Ti-Si-based intermetallic compounds in addition to the aforementioned phases. The study found that the Si-added alloy had a greater quantity of T phase in comparison to the base alloy, which was attributed to the promotion of T phase precipitation facilitated by the inclusion of Si. Additionally, Si facilitated the formation of S phase during aging treatment, thereby accelerating the precipitation-hardening response of the Si-added alloy. The as-cast temper of the base alloy displayed a yield strength of roughly 153 MPa, which increased to 170 MPa in the Si-added alloy. As a result of the aging treatment, both alloys exhibited a notable increase in tensile strength, which was ascribed to the precipitation of S phases. In the T6 temper, the base alloy exhibited a yield strength of 270 MPa, while the Si-added alloy exhibited a significantly higher yield strength of 324 MPa. This novel Si-added alloy demonstrated superior tensile properties compared to many commercially available high-Mg-added Al–Cu–Mg alloys, making it a potential replacement for such alloys in various applications within the aerospace and automotive industries.