Growth Dynamics of Ultrathin Films of Benzo[1,2-b:4,5-b’]dithiophene Derivatives on Au(111): A Photoelectron Spectroscopy Investigation

[Image: see text] Ultrathin films of a stereoisomeric mixture of benzo[1,2-b:4,5-b’]dithiophene derivatives were grown by thermal evaporation in vacuum on Au(111), and they were studied in situ by photoelectron spectroscopy. X-ray photons from a non-monochromatic Mg Kα conventional X-ray source and...

Descripción completa

Detalles Bibliográficos
Autores principales: Stummo, Angelo, Montecchi, Monica, Parenti, Francesca, Vanossi, Davide, Fontanesi, Claudio, Capelli, Raffaella, Pasquali, Luca
Formato: Online Artículo Texto
Lenguaje:English
Publicado: American Chemical Society 2023
Acceso en línea:https://www.ncbi.nlm.nih.gov/pmc/articles/PMC10116645/
https://www.ncbi.nlm.nih.gov/pubmed/37027516
http://dx.doi.org/10.1021/acs.langmuir.3c00572
Descripción
Sumario:[Image: see text] Ultrathin films of a stereoisomeric mixture of benzo[1,2-b:4,5-b’]dithiophene derivatives were grown by thermal evaporation in vacuum on Au(111), and they were studied in situ by photoelectron spectroscopy. X-ray photons from a non-monochromatic Mg Kα conventional X-ray source and UV photons from a He I discharge lamp equipped with a linear polarizer were used. He I photoemission results were compared with density functional theory (DFT) calculations: density of states (DOS) and 3D molecular orbital density distribution. Au 4f, C 1s, O 1s, and S 2p core-level components suggest a surface rearrangement as a function of film nominal thickness, with the variation of the molecular orientation, from flat-laying at the initial deposition to tilted toward the surface normal at coverages exceeding 2 nm. Eventually, the DFT results were exploited in assigning of the valence band experimental structures. Moreover, polarization-dependent photoemission confirmed the tilted arrangement of the molecules, starting at 2 nm. A variation of the work function of 1.4 eV with respect to the clean substrate was measured, together with a valence band offset of 1.3 eV between the organic layer and gold.