Cargando…

Power dependent photoacoustic and photoluminescence studies on a Ho(3+)/Yb(3+) doped Y(2)O(3) phosphor

The Ho(3+)/Yb(3+) doped Y(2)O(3) phosphor samples were synthesized through a combustion method and then were annealed at 800 °C, 1000 °C, and 1200 °C. The cubic phase of the synthesized samples was confirmed by XRD analysis. The upconversion (UC) & photoacoustic (PA) spectroscopic studies were d...

Descripción completa

Detalles Bibliográficos
Autores principales: Sarkar, Minarul I., Kumar, Kaushal
Formato: Online Artículo Texto
Lenguaje:English
Publicado: The Royal Society of Chemistry 2023
Materias:
Acceso en línea:https://www.ncbi.nlm.nih.gov/pmc/articles/PMC10126742/
https://www.ncbi.nlm.nih.gov/pubmed/37114027
http://dx.doi.org/10.1039/d3ra00643c