Effect of Mg Contents on the Microstructure, Mechanical Properties and Cytocompatibility of Degradable Zn-0.5Mn-xMg Alloy

The effect of magnesium (Mg) content on the microstructure, mechanical properties, and cytocompatibility of degradable Zn-0.5Mn-xMg (x = 0.05 wt%, 0.2 wt%, 0.5 wt%) alloys was investigated. The microstructure, corrosion products, mechanical properties, and corrosion properties of the three alloys we...

Descripción completa

Detalles Bibliográficos
Autores principales: Yang, Lingbo, Li, Xing, Yang, Lijing, Zhu, Xinglong, Wang, Manli, Song, Zhenlun, Liu, Huinan Hannah, Sun, Wensheng, Dong, Ruihong, Yue, Jiqiang
Formato: Online Artículo Texto
Lenguaje:English
Publicado: MDPI 2023
Materias:
Acceso en línea:https://www.ncbi.nlm.nih.gov/pmc/articles/PMC10145424/
https://www.ncbi.nlm.nih.gov/pubmed/37103285
http://dx.doi.org/10.3390/jfb14040195
Descripción
Sumario:The effect of magnesium (Mg) content on the microstructure, mechanical properties, and cytocompatibility of degradable Zn-0.5Mn-xMg (x = 0.05 wt%, 0.2 wt%, 0.5 wt%) alloys was investigated. The microstructure, corrosion products, mechanical properties, and corrosion properties of the three alloys were then thoroughly characterized by scanning electron microscopy (SEM), electron back-scattered diffraction (EBSD), and other methods. According to the findings, the grain size of matrix was refined by the addition of Mg, while the size and quantity of Mg(2)Zn(11) phase was increased. The Mg content could significantly improve the ultimate tensile strength (UTS) of the alloy. Compared with the Zn-0.5Mn alloy, the UTS of Zn-0.5Mn-xMg alloy was increased significantly. Zn-0.5Mn-0.5Mg exhibited the highest UTS (369.6 MPa). The strength of the alloy was influenced by the average grain size, the solid solubility of Mg, and the quantity of Mg(2)Zn(11) phase. The increase in the quantity and size of Mg(2)Zn(11) phase was the main reason for the transition from ductile fracture to cleavage fracture. Moreover, Zn-0.5Mn-0.2Mg alloy showed the best cytocompatibility to L-929 cells.