Ultra-Sensitive and Fast Humidity Sensors Based on Direct Laser-Scribed Graphene Oxide/Carbon Nanotubes Composites

In this paper, the relative humidity sensor properties of graphene oxide (GO) and graphene oxide/multiwalled nanotubes (GO/MWNTs) composites have been investigated. Composite sensors were fabricated by direct laser scribing and characterized using UV-vis-NIR, Raman, Fourier transform infrared, and X...

Descripción completa

Detalles Bibliográficos
Autores principales: Al-Hamry, Ammar, Lu, Tianqi, Chen, Haoran, Adiraju, Anurag, Nasraoui, Salem, Brahem, Amina, Bajuk-Bogdanović, Danica, Weheabby, Saddam, Pašti, Igor A., Kanoun, Olfa
Formato: Online Artículo Texto
Lenguaje:English
Publicado: MDPI 2023
Materias:
Acceso en línea:https://www.ncbi.nlm.nih.gov/pmc/articles/PMC10180099/
https://www.ncbi.nlm.nih.gov/pubmed/37177018
http://dx.doi.org/10.3390/nano13091473
Descripción
Sumario:In this paper, the relative humidity sensor properties of graphene oxide (GO) and graphene oxide/multiwalled nanotubes (GO/MWNTs) composites have been investigated. Composite sensors were fabricated by direct laser scribing and characterized using UV-vis-NIR, Raman, Fourier transform infrared, and X-ray photoemission spectroscopies, electron scanning microscopy coupled with energy-dispersive X-ray analysis, and impedance spectroscopy (IS). These methods confirm the composite homogeneity and laser reduction of GO/MWNT with dominant GO characteristics, while ISresults analysis reveals the circuit model for rGO-GO-rGO structure and the effect of MWNT on the sensor properties. Although direct laser scribing of GO-based humidity sensor shows an outstanding response (|ΔZ|/|Z| up to 638,800%), a lack of stability and repeatability has been observed. GO/MWNT-based humidity sensors are more conductive than GO sensors and relatively less sensitive (|ΔZ|/|Z| = 163,000%). However, they are more stable in harsh humid conditions, repeatable, and reproducible even after several years of shelf-life. In addition, they have fast response/recovery times of 10.7 s and 9.3 s and an ultra-fast response time of 61 ms when abrupt humidification/dehumidification is applied by respiration. All carbon-based sensors’ overall properties confirm the advantage of introducing the GO/MWNT hybrid and laser direct writing to produce stable structures and sensors.