Improvement of Hot Tearing Resistance of AZ91 Alloy with the Addition of Trace Ca
Hot tearing is the most common and serious casting defect that restricts the light weight and integration of magnesium alloy components. In the present study, trace Ca (0–1.0 wt.%) was added to improve the resistance of AZ91 alloy to hot tearing. The hot tearing susceptivity (HTS) of alloys was expe...
Autores principales: | Xiang, Hongchen, Liu, Wenjun, Wang, Qiang, Jiang, Bin, Song, Jiangfeng, Wu, Hang, Feng, Nan, Chai, Linjiang |
---|---|
Formato: | Online Artículo Texto |
Lenguaje: | English |
Publicado: |
MDPI
2023
|
Materias: | |
Acceso en línea: | https://www.ncbi.nlm.nih.gov/pmc/articles/PMC10220820/ https://www.ncbi.nlm.nih.gov/pubmed/37241513 http://dx.doi.org/10.3390/ma16103886 |
Ejemplares similares
-
Linear Friction Welding of an AZ91 Magnesium Alloy and the Effect of Ca Additions on the Weld Characteristics
por: Villegas-Armenta, Luis Angel, et al.
Publicado: (2021) -
Effect of SiC Nanoparticles on Hot Deformation Behavior and Processing Maps of Magnesium Alloy AZ91
por: Nie, Kaibo, et al.
Publicado: (2018) -
Cerium Addition Improved the Dry Sliding Wear Resistance of Surface Welding AZ91 Alloy
por: Chen, Qingqiang, et al.
Publicado: (2018) -
Influence of Rare Earth Element (Y) on Microstructure and Corrosion Behavior of Hot Extrusion AZ91 Magnesium Alloy
por: Cui, Yanan, et al.
Publicado: (2020) -
Comprehensive Research of FSW Joints of AZ91 Magnesium Alloy
por: Mroczka, Krzysztof, et al.
Publicado: (2023)