Preparation and Modification of Polydopamine Boron Nitride—Titanium Dioxide Nanohybrid Particles Incorporated into Zinc Phosphating Bath to Enhance Corrosion Performance of Zinc Phosphate-Silane Coated Q235 Steel
In this work, PDA@BN-TiO(2) nanohybrid particles were incorporated chemically into a zinc-phosphating solution to form a robust, low-temperature phosphate-silane coating on Q235 steel specimens. The morphology and surface modification of the coating was characterized by X-Ray Diffraction (XRD), X-ra...
Autores principales: | , , , , , |
---|---|
Formato: | Online Artículo Texto |
Lenguaje: | English |
Publicado: |
MDPI
2023
|
Materias: | |
Acceso en línea: | https://www.ncbi.nlm.nih.gov/pmc/articles/PMC10221017/ https://www.ncbi.nlm.nih.gov/pubmed/37241462 http://dx.doi.org/10.3390/ma16103835 |
Sumario: | In this work, PDA@BN-TiO(2) nanohybrid particles were incorporated chemically into a zinc-phosphating solution to form a robust, low-temperature phosphate-silane coating on Q235 steel specimens. The morphology and surface modification of the coating was characterized by X-Ray Diffraction (XRD), X-ray Spectroscopy (XPS), Fourier-transform infrared spectroscopy (FT-IR), and Scanning electron microscopy (SEM). Results demonstrate that the incorporation of PDA@BN-TiO(2) nanohybrids produced a higher number of nucleation sites and reduced grain size with a denser, more robust, and more corrosion-resistant phosphate coating compared to pure coating. The coating weight results showed that the PBT-0.3 sample achieved the densest and most uniform coating (38.2 g/m(2)). The potentiodynamic polarization results showed that the PDA@BN-TiO(2) nanohybrid particles increased phosphate-silane films’ homogeneity and anti-corrosive capabilities. The 0.3 g/L sample exhibits the best performance with an electric current density of 1.95 × 10(−5) A/cm(2), an order of magnitude lower than that of the pure coatings. Electrochemical impedance spectroscopy revealed that PDA@BN-TiO(2) nanohybrids provided the greatest corrosion resistance compared to pure coatings. The corrosion time for copper sulfate in samples containing PDA@BN/TiO(2) prolonged to 285 s, a significantly higher amount of time than the corrosion time found in pure samples. |
---|