Thermoplastic elastomers based on recycled high-density polyethylene/ground tire rubber/ethylene vinyl acetate: Effect of ground tire rubber regeneration on morphological and mechanical properties

This work investigates the properties of different types of regenerated recycled rubbers (RR(1) and RR(2)) to produce thermoplastic elastomers (TPE) based on recycled high-density polyethylene (RHD) as the matrix. The higher regeneration degree of RR(2) (24%) compared to RR(1) (15%) was able to bett...

Descripción completa

Detalles Bibliográficos
Autores principales: Fazli, Ali, Rodrigue, Denis
Formato: Online Artículo Texto
Lenguaje:English
Publicado: SAGE Publications 2022
Materias:
Acceso en línea:https://www.ncbi.nlm.nih.gov/pmc/articles/PMC10235528/
https://www.ncbi.nlm.nih.gov/pubmed/37275338
http://dx.doi.org/10.1177/08927057221095388
Descripción
Sumario:This work investigates the properties of different types of regenerated recycled rubbers (RR(1) and RR(2)) to produce thermoplastic elastomers (TPE) based on recycled high-density polyethylene (RHD) as the matrix. The higher regeneration degree of RR(2) (24%) compared to RR(1) (15%) was able to better restore the plasticity and processability of the ground tire rubber (GTR). So better entanglement between RR(2) free chains and the thermoplastic macromolecules was obtained inducing stronger interfacial interaction leading to higher elongation at break (159%) and impact strength (342 J/m) of the blends filled with 80 wt.% RR(2). To further improve the adhesion and achieve rubber-like properties, ethylene vinyl acetate (EVA) was used as a compatibilizer. The microstructure analysis showed that uniform dispersion of the particles and ground tire rubber encapsulation by EVA increased the resistance to crack propagation and failure of the compatibilized blends. The swelling, mechanical and physical properties of the ternary blends (RHD/GTR/EVA) showed that EVA improved the interfacial interactions between GTR and RHD which was confirmed by enhanced elongation at break (203%) and impact strength (379 J/m) by the addition of 10 wt.% EVA.