Objectives: This study aimed to assess the microtensile bond strength (µTBS) of etch-and-rinse (E&R), self-etch (SE), and universal adhesives to superficial and deep dentin. Materials and Methods: In this in vitro study, 40 sound third molars were randomly divided into two main groups of superfi...

Descripción completa

Detalles Bibliográficos
Autores principales: Sharifian, Atefe, Esmaeili, Behnaz, Gholinia, Hemmat, Ezoji, Fariba
Formato: Online Artículo Texto
Lenguaje:English
Publicado: Tehran University of Medical Sciences 2023
Materias:
Acceso en línea:https://www.ncbi.nlm.nih.gov/pmc/articles/PMC10258392/
https://www.ncbi.nlm.nih.gov/pubmed/37312827
http://dx.doi.org/10.18502/fid.v20i9.12608
_version_ 1785057456645210112
author Sharifian, Atefe
Esmaeili, Behnaz
Gholinia, Hemmat
Ezoji, Fariba
author_facet Sharifian, Atefe
Esmaeili, Behnaz
Gholinia, Hemmat
Ezoji, Fariba
author_sort Sharifian, Atefe
collection PubMed
description Objectives: This study aimed to assess the microtensile bond strength (µTBS) of etch-and-rinse (E&R), self-etch (SE), and universal adhesives to superficial and deep dentin. Materials and Methods: In this in vitro study, 40 sound third molars were randomly divided into two main groups of superficial and deep dentin. Based on our classification, superficial dentin was right beneath the deepest occlusal groove, and deep dentin was 2mm beneath the deepest occlusal groove. Each group was divided into 4 subgroups (n=20) for application of Adper Single Bond 2 (ASB), Clearfil SE Bond (CSE), and Scotchbond Universal (SBU) in E&R and SE modes along with Charisma Smart composite resin on dentin. The specimens were incubated in distilled water at 37°C for 24 hours and their µTBS was then measured. The mode of failure was determined under a stereomicroscope at ×40 magnification. Data were analyzed by one-way ANOVA (alpha=0.05). Results: The highest µTBS belonged to the superficial dentin/SBU/E&R group. The µTBS was significantly higher in superficial dentin than deep dentin for all adhesives (P=0.005). There was no significant difference in mode of failure among the groups. Conclusion: Based on the results obtained in the present study, type of bonding agent and application mode affected µTBS. In use of universal adhesive, E&R mode can improve µTBS.
format Online
Article
Text
id pubmed-10258392
institution National Center for Biotechnology Information
language English
publishDate 2023
publisher Tehran University of Medical Sciences
record_format MEDLINE/PubMed
spelling pubmed-102583922023-06-13 Microtensile Bond Strength of Different Bonding Agents to Superficial and Deep Dentin in Etch-and-Rinse and Self-Etch Modes Sharifian, Atefe Esmaeili, Behnaz Gholinia, Hemmat Ezoji, Fariba Front Dent Original Article Objectives: This study aimed to assess the microtensile bond strength (µTBS) of etch-and-rinse (E&R), self-etch (SE), and universal adhesives to superficial and deep dentin. Materials and Methods: In this in vitro study, 40 sound third molars were randomly divided into two main groups of superficial and deep dentin. Based on our classification, superficial dentin was right beneath the deepest occlusal groove, and deep dentin was 2mm beneath the deepest occlusal groove. Each group was divided into 4 subgroups (n=20) for application of Adper Single Bond 2 (ASB), Clearfil SE Bond (CSE), and Scotchbond Universal (SBU) in E&R and SE modes along with Charisma Smart composite resin on dentin. The specimens were incubated in distilled water at 37°C for 24 hours and their µTBS was then measured. The mode of failure was determined under a stereomicroscope at ×40 magnification. Data were analyzed by one-way ANOVA (alpha=0.05). Results: The highest µTBS belonged to the superficial dentin/SBU/E&R group. The µTBS was significantly higher in superficial dentin than deep dentin for all adhesives (P=0.005). There was no significant difference in mode of failure among the groups. Conclusion: Based on the results obtained in the present study, type of bonding agent and application mode affected µTBS. In use of universal adhesive, E&R mode can improve µTBS. Tehran University of Medical Sciences 2023-04-30 /pmc/articles/PMC10258392/ /pubmed/37312827 http://dx.doi.org/10.18502/fid.v20i9.12608 Text en Copyright © 2023 The Authors. Published by Tehran University of Medical Sciences. https://creativecommons.org/licenses/by-nc/4.0/This work is licensed under a Creative Commons Attribution-NonCommercial 4.0 International license (https://creativecommons.org/licenses/by-nc/4.0/). Non-commercial uses of the work are permitted, provided the original work is properly cited.
spellingShingle Original Article
Sharifian, Atefe
Esmaeili, Behnaz
Gholinia, Hemmat
Ezoji, Fariba
Microtensile Bond Strength of Different Bonding Agents to Superficial and Deep Dentin in Etch-and-Rinse and Self-Etch Modes
title Microtensile Bond Strength of Different Bonding Agents to Superficial and Deep Dentin in Etch-and-Rinse and Self-Etch Modes
title_full Microtensile Bond Strength of Different Bonding Agents to Superficial and Deep Dentin in Etch-and-Rinse and Self-Etch Modes
title_fullStr Microtensile Bond Strength of Different Bonding Agents to Superficial and Deep Dentin in Etch-and-Rinse and Self-Etch Modes
title_full_unstemmed Microtensile Bond Strength of Different Bonding Agents to Superficial and Deep Dentin in Etch-and-Rinse and Self-Etch Modes
title_short Microtensile Bond Strength of Different Bonding Agents to Superficial and Deep Dentin in Etch-and-Rinse and Self-Etch Modes
title_sort microtensile bond strength of different bonding agents to superficial and deep dentin in etch-and-rinse and self-etch modes
topic Original Article
url https://www.ncbi.nlm.nih.gov/pmc/articles/PMC10258392/
https://www.ncbi.nlm.nih.gov/pubmed/37312827
http://dx.doi.org/10.18502/fid.v20i9.12608
work_keys_str_mv AT sharifianatefe microtensilebondstrengthofdifferentbondingagentstosuperficialanddeepdentininetchandrinseandselfetchmodes
AT esmaeilibehnaz microtensilebondstrengthofdifferentbondingagentstosuperficialanddeepdentininetchandrinseandselfetchmodes
AT gholiniahemmat microtensilebondstrengthofdifferentbondingagentstosuperficialanddeepdentininetchandrinseandselfetchmodes
AT ezojifariba microtensilebondstrengthofdifferentbondingagentstosuperficialanddeepdentininetchandrinseandselfetchmodes