Origin of Heterogeneous Stripping of Lithium in Liquid Electrolytes

[Image: see text] Lithium metal batteries suffer from low cycle life. During discharge, parts of the lithium are not stripped reversibly and remain isolated from the current collector. This isolated lithium is trapped in the insulating remaining solid-electrolyte interphase (SEI) shell and contribut...