A cost-effective, ionically conductive and compressible oxychloride solid-state electrolyte for stable all-solid-state lithium-based batteries
To enable the development of all-solid-state batteries, an inorganic solid-state electrolyte should demonstrate high ionic conductivity (i.e., > 1 mS cm(−1) at 25 °C), compressibility (e.g., > 90% density under 250−350 MPa), and cost-effectiveness (e.g., < $50/kg). Here we report the develo...
Autores principales: | , , , , , , , , , |
---|---|
Formato: | Online Artículo Texto |
Lenguaje: | English |
Publicado: |
Nature Publishing Group UK
2023
|
Materias: | |
Acceso en línea: | https://www.ncbi.nlm.nih.gov/pmc/articles/PMC10300059/ https://www.ncbi.nlm.nih.gov/pubmed/37369677 http://dx.doi.org/10.1038/s41467-023-39522-1 |
Sumario: | To enable the development of all-solid-state batteries, an inorganic solid-state electrolyte should demonstrate high ionic conductivity (i.e., > 1 mS cm(−1) at 25 °C), compressibility (e.g., > 90% density under 250−350 MPa), and cost-effectiveness (e.g., < $50/kg). Here we report the development and preparation of Li(1.75)ZrCl(4.75)O(0.5) oxychloride solid-state electrolyte that demonstrates an ionic conductivity of 2.42 mS cm(−1) at 25 °C, a compressibility enabling 94.2% density under 300 MPa and an estimated raw materials cost of $11.60/kg. As proof of concept, the Li(1.75)ZrCl(4.75)O(0.5) is tested in combination with a LiNi(0.8)Mn(0.1)Co(0.1)O(2)-based positive electrode and a Li(6)PS(5)Cl-coated Li-In negative electrode in lab-scale cell configuration. This all-solid-state cell delivers a discharge capacity retention of 70.34% (final discharge capacity of 70.2 mAh g(−1)) after 2082 cycles at 1 A g(−1), 25 °C and 1.5 tons of stacking pressure. |
---|