Performance Optimization of Pb(0.97)La(0.03)Sc(0.45)Ta(0.45)Ti(0.1)O(3) Ceramics by Annealing Process
The annealing effects on Pb(0.97)La(0.03)Sc(0.45)Ta(0.45)Ti(0.1)O(3) (PLSTT) ceramics prepared by the solid-state reaction method are systemically investigated using experimental and theoretical techniques. Comprehensive studies are performed on the PLSTT samples by varying annealing time (AT) from...
Autores principales: | Su, Zihan, Wan, Lingyu, Mo, Fenglai, Li, Jiayu, Liu, Boxun, Liang, Chuangjian, Xu, Jinsong, Talwar, Devki N., Li, Hang, Yao, Huilu |
---|---|
Formato: | Online Artículo Texto |
Lenguaje: | English |
Publicado: |
MDPI
2023
|
Materias: | |
Acceso en línea: | https://www.ncbi.nlm.nih.gov/pmc/articles/PMC10305350/ https://www.ncbi.nlm.nih.gov/pubmed/37374662 http://dx.doi.org/10.3390/ma16124479 |
Ejemplares similares
-
Ocular pharmacokinetics of 0.45% ketorolac tromethamine
por: Attar, Mayssa, et al.
Publicado: (2010) -
In vitro and in vivo degradation behavior of Mg-0.45Zn-0.45Ca (ZX00) screws for orthopedic applications
por: Martinez, Diana C., et al.
Publicado: (2023) -
Metal-Semiconductor AsSb-Al(0.6)Ga(0.4)As(0.97)Sb(0.03) Metamaterial
por: Bert, Nikolay, et al.
Publicado: (2022) -
Si(0.97)Ge(0.03) microelectronic thermoelectric generators with high power and voltage densities
por: Dhawan, Ruchika, et al.
Publicado: (2020) -
Anomalous behavior above the Curie temperature in (Nd(1−x)Gd(x))(0.55)Sr(0.45)MnO(3) (x = 0, 0.1, 0.3 and 0.5)
por: Kamel, R., et al.
Publicado: (2019)