Microstructural Evolution, Mechanical Properties and Tribological Behavior of B(4)C-Reinforced Ti In Situ Composites Produced by Laser Powder Bed Fusion
Based on the advantage of rapid net-shape fabrication, laser powder bed fusion (LPBF) is utilized to process B(4)C-reinforced Ti composites. The effect of volumetric energy density (VED) on the relative density, microstructural evolution, tensile properties and wear behaviors of B(4)C-reinforced Ti...
Autores principales: | , , , , , , , |
---|---|
Formato: | Online Artículo Texto |
Lenguaje: | English |
Publicado: |
MDPI
2023
|
Materias: | |
Acceso en línea: | https://www.ncbi.nlm.nih.gov/pmc/articles/PMC10343199/ https://www.ncbi.nlm.nih.gov/pubmed/37445205 http://dx.doi.org/10.3390/ma16134890 |
Sumario: | Based on the advantage of rapid net-shape fabrication, laser powder bed fusion (LPBF) is utilized to process B(4)C-reinforced Ti composites. The effect of volumetric energy density (VED) on the relative density, microstructural evolution, tensile properties and wear behaviors of B(4)C-reinforced Ti composites were systematically investigated. The LPBF-ed samples with high relative density (>99%) can be achieved, while the pores and un-melted powders can be observed in the sample owing to the low energy input (33 J/mm(3)). The additive particulates B(4)C were transformed into needle-like TiB whiskers with nano-scale while C dissolved in the Ti matrix. Fine-scale grains (<10 μm) with random crystallographic orientation can be achieved and the residual stress shows a downtrend as the VED increases. Through the analysis of the tensile and wear tests, the sample at 61 J/mm(3) VED showed a good combination of strength and wear performance, with an ultimate tensile strength of 951 MPa and a wear rate of 3.91 × 10(−4) mm(3)·N(−1)m(−1). The microstructural evolution in VED changes and the corresponding underlying strengthening mechanisms of LPBF-ed Ti + B(4)C composites are conducted in detail. |
---|