Biosorption of Escherichia coli Using ZnO-Trimethyl Chitosan Nanocomposite Hydrogel Formed by the Green Synthesis Route

In this study, we tested the biosorption capacity of trimethyl chitosan (TMC)-ZnO nanocomposite (NC) for the adsorptive removal of Escherichia coli (E. coli) in aqueous suspension. For the formation of ZnO NPs, we followed the green synthesis route involving Terminalia mantaly (TM) aqueous leaf extr...

Descripción completa

Detalles Bibliográficos
Autores principales: Bwatanglang, Ibrahim Birma, Mohammad, Faruq, Janet, John Nahadi, Dahan, Wasmia Mohammed, Al-Lohedan, Hamad A., Soleiman, Ahmed A.
Formato: Online Artículo Texto
Lenguaje:English
Publicado: MDPI 2023
Materias:
Acceso en línea:https://www.ncbi.nlm.nih.gov/pmc/articles/PMC10378975/
https://www.ncbi.nlm.nih.gov/pubmed/37504460
http://dx.doi.org/10.3390/gels9070581
_version_ 1785079898657783808
author Bwatanglang, Ibrahim Birma
Mohammad, Faruq
Janet, John Nahadi
Dahan, Wasmia Mohammed
Al-Lohedan, Hamad A.
Soleiman, Ahmed A.
author_facet Bwatanglang, Ibrahim Birma
Mohammad, Faruq
Janet, John Nahadi
Dahan, Wasmia Mohammed
Al-Lohedan, Hamad A.
Soleiman, Ahmed A.
author_sort Bwatanglang, Ibrahim Birma
collection PubMed
description In this study, we tested the biosorption capacity of trimethyl chitosan (TMC)-ZnO nanocomposite (NC) for the adsorptive removal of Escherichia coli (E. coli) in aqueous suspension. For the formation of ZnO NPs, we followed the green synthesis route involving Terminalia mantaly (TM) aqueous leaf extract as a reducing agent, and the formed ZnO particles were surface-coated with TMC biopolymer. On testing of the physicochemical characteristics, the TM@ZnO/TMC (NC) hydrogel showed a random spherical morphology with an average size of 31.8 ± 2.6 nm and a crystal size of 28.0 ± 7.7 nm. The zeta potential of the composite was measured to be 23.5 mV with a BET surface area of 3.01 m(2) g(−1). The spectral profiles of TM@ZnO/TMC NC hydrogel on interaction with Escherichia coli (E. coli) revealed some conformational changes to the functional groups assigned to the stretching vibrations of N-H, C-O-C, C-O ring, and C=O bonds. The adsorption kinetics of TM@ZnO/TMC NC hydrogel revealed the pseudo-second-order as the best fit mechanism for the E. coli biosorption. The surface homogeneity and monolayer adsorption of the TM@ZnO/TMC NC hydrogel reflects majorly the entire adsorption mechanism, observed to display the highest correlation for Jovanovic, Redlich–Peterson, and Langmuir’s isotherm models. Further, with the use of TM@ZnO/TMC NC hydrogel, we measured the highest adsorption capacity of E. coli to be 4.90 × 10 mg g(−1), where an in-depth mechanistic pathway was proposed by making use of the FTIR analysis.
format Online
Article
Text
id pubmed-10378975
institution National Center for Biotechnology Information
language English
publishDate 2023
publisher MDPI
record_format MEDLINE/PubMed
spelling pubmed-103789752023-07-29 Biosorption of Escherichia coli Using ZnO-Trimethyl Chitosan Nanocomposite Hydrogel Formed by the Green Synthesis Route Bwatanglang, Ibrahim Birma Mohammad, Faruq Janet, John Nahadi Dahan, Wasmia Mohammed Al-Lohedan, Hamad A. Soleiman, Ahmed A. Gels Article In this study, we tested the biosorption capacity of trimethyl chitosan (TMC)-ZnO nanocomposite (NC) for the adsorptive removal of Escherichia coli (E. coli) in aqueous suspension. For the formation of ZnO NPs, we followed the green synthesis route involving Terminalia mantaly (TM) aqueous leaf extract as a reducing agent, and the formed ZnO particles were surface-coated with TMC biopolymer. On testing of the physicochemical characteristics, the TM@ZnO/TMC (NC) hydrogel showed a random spherical morphology with an average size of 31.8 ± 2.6 nm and a crystal size of 28.0 ± 7.7 nm. The zeta potential of the composite was measured to be 23.5 mV with a BET surface area of 3.01 m(2) g(−1). The spectral profiles of TM@ZnO/TMC NC hydrogel on interaction with Escherichia coli (E. coli) revealed some conformational changes to the functional groups assigned to the stretching vibrations of N-H, C-O-C, C-O ring, and C=O bonds. The adsorption kinetics of TM@ZnO/TMC NC hydrogel revealed the pseudo-second-order as the best fit mechanism for the E. coli biosorption. The surface homogeneity and monolayer adsorption of the TM@ZnO/TMC NC hydrogel reflects majorly the entire adsorption mechanism, observed to display the highest correlation for Jovanovic, Redlich–Peterson, and Langmuir’s isotherm models. Further, with the use of TM@ZnO/TMC NC hydrogel, we measured the highest adsorption capacity of E. coli to be 4.90 × 10 mg g(−1), where an in-depth mechanistic pathway was proposed by making use of the FTIR analysis. MDPI 2023-07-17 /pmc/articles/PMC10378975/ /pubmed/37504460 http://dx.doi.org/10.3390/gels9070581 Text en © 2023 by the authors. https://creativecommons.org/licenses/by/4.0/Licensee MDPI, Basel, Switzerland. This article is an open access article distributed under the terms and conditions of the Creative Commons Attribution (CC BY) license (https://creativecommons.org/licenses/by/4.0/).
spellingShingle Article
Bwatanglang, Ibrahim Birma
Mohammad, Faruq
Janet, John Nahadi
Dahan, Wasmia Mohammed
Al-Lohedan, Hamad A.
Soleiman, Ahmed A.
Biosorption of Escherichia coli Using ZnO-Trimethyl Chitosan Nanocomposite Hydrogel Formed by the Green Synthesis Route
title Biosorption of Escherichia coli Using ZnO-Trimethyl Chitosan Nanocomposite Hydrogel Formed by the Green Synthesis Route
title_full Biosorption of Escherichia coli Using ZnO-Trimethyl Chitosan Nanocomposite Hydrogel Formed by the Green Synthesis Route
title_fullStr Biosorption of Escherichia coli Using ZnO-Trimethyl Chitosan Nanocomposite Hydrogel Formed by the Green Synthesis Route
title_full_unstemmed Biosorption of Escherichia coli Using ZnO-Trimethyl Chitosan Nanocomposite Hydrogel Formed by the Green Synthesis Route
title_short Biosorption of Escherichia coli Using ZnO-Trimethyl Chitosan Nanocomposite Hydrogel Formed by the Green Synthesis Route
title_sort biosorption of escherichia coli using zno-trimethyl chitosan nanocomposite hydrogel formed by the green synthesis route
topic Article
url https://www.ncbi.nlm.nih.gov/pmc/articles/PMC10378975/
https://www.ncbi.nlm.nih.gov/pubmed/37504460
http://dx.doi.org/10.3390/gels9070581
work_keys_str_mv AT bwatanglangibrahimbirma biosorptionofescherichiacoliusingznotrimethylchitosannanocompositehydrogelformedbythegreensynthesisroute
AT mohammadfaruq biosorptionofescherichiacoliusingznotrimethylchitosannanocompositehydrogelformedbythegreensynthesisroute
AT janetjohnnahadi biosorptionofescherichiacoliusingznotrimethylchitosannanocompositehydrogelformedbythegreensynthesisroute
AT dahanwasmiamohammed biosorptionofescherichiacoliusingznotrimethylchitosannanocompositehydrogelformedbythegreensynthesisroute
AT allohedanhamada biosorptionofescherichiacoliusingznotrimethylchitosannanocompositehydrogelformedbythegreensynthesisroute
AT soleimanahmeda biosorptionofescherichiacoliusingznotrimethylchitosannanocompositehydrogelformedbythegreensynthesisroute