Optimization of the Methods to Develop Stable Polymer Gels for Water Management in Medium- and Ultra-High-Salinity Reservoirs
Polymer gels suffer from a serious syneresis issue when exposed to high-temperature and high-salinity (HTHS) conditions, which limits their use as water-treatment agents in this type of reservoir. In this paper, the effects of the polymer type/concentration, deoxidizers, and stabilizers on the long-...
Autores principales: | , , , , |
---|---|
Formato: | Online Artículo Texto |
Lenguaje: | English |
Publicado: |
MDPI
2023
|
Materias: | |
Acceso en línea: | https://www.ncbi.nlm.nih.gov/pmc/articles/PMC10379814/ https://www.ncbi.nlm.nih.gov/pubmed/37504419 http://dx.doi.org/10.3390/gels9070540 |
Sumario: | Polymer gels suffer from a serious syneresis issue when exposed to high-temperature and high-salinity (HTHS) conditions, which limits their use as water-treatment agents in this type of reservoir. In this paper, the effects of the polymer type/concentration, deoxidizers, and stabilizers on the long-term stability of polymer gels were systematically studied; thus, the methods to develop stable polymer gels for two typical levels of salinity were optimized. The results show the following: (1) For a medium-salinity condition (TDS: 33,645.0 mg/L) at 125 °C, conventional HPAM gels completely dehydrate within only 1 day, and the addition of a deoxidizer hardly improved their stability. Some special polymers, e.g., AP-P5, MKY, and CPAM, are able to form stable gels if a high concentration of 0.8% is used; the syneresis rate of these gels is about 10% after 30 days. However, the addition of the complexant sodium oxalate significantly improves the stability of gels formed by all five of these different polymers, which behave with a 0% syneresis rate after 30 days pass. Complexants are the most economical and feasible agents to develop stable gels in medium-salinity water. (2) Gels enhanced using the methods above all become unstable in a more challenging ultra-high-saline condition (TDS: 225,068.0 mg/L). In this case, special calcium- and magnesium-resistant polymers are required to prepare stable gels, which show 0% syneresis rates after 30 days, have relatively low strengths, but do produce a good plugging effect in high-permeability cores. |
---|