Effect of a 3.5% NaCl−10% HCl Corrosive Environment on the Fatigue Behavior of Hot Rolled Aluminum 5083-H111
This study deals with the microstructure of rolled Al5083-H111 materials, their hardness, corrosion in different solutions, and rotary bending fatigue properties of non-corroded and corroded samples in different solutions. This study is the first to report the fatigue behavior of corroded samples in...
Autores principales: | Elhasslouk, Masoud M. M., Esen, İsmail, Ahlatcı, Hayrettin, Akın, Bengu |
---|---|
Formato: | Online Artículo Texto |
Lenguaje: | English |
Publicado: |
MDPI
2023
|
Materias: | |
Acceso en línea: | https://www.ncbi.nlm.nih.gov/pmc/articles/PMC10384590/ https://www.ncbi.nlm.nih.gov/pubmed/37512270 http://dx.doi.org/10.3390/ma16144996 |
Ejemplares similares
-
Evolution of the Corrosion Product Film on Nickel-Aluminum Bronze and Its Corrosion Behavior in 3.5 wt % NaCl Solution
por: Ding, Yang, et al.
Publicado: (2019) -
Electrochemical data of single and hybrid sol–gel coating precursors for aluminum alloy corrosion protection in 3.5% NaCl
por: Hussin, M. Hazwan
Publicado: (2019) -
The Corrosion Resistance of Reinforced Reactive Powder Concrete with Secondary Aluminum Ash Exposed to NaCl Action
por: Jiang, Hong, et al.
Publicado: (2023) -
Investigation of the Hot Stamping-in-Die Quenching Composite Forming Process of 5083 Aluminum Alloy Skin
por: Yi, Lingling, et al.
Publicado: (2023) -
Examination of the Corrosion Behavior of Shape Memory NiTi Material for Biomedical Applications
por: Soltan, Aboujaila A. M., et al.
Publicado: (2023)