Does repeated autoclave sterilization cause changes in the color and fragility of fiberglass reinforced resin crowns?
BACKGROUND: Since the effects of sterilization on the Fiberglass Reinforced Resin Crowns (FRRCs) is not well-known the aim of current study was to evaluate the effects of autoclave sterilization on the fracture resistance, color stability, and surface composition of FRRCs. METHODS: A total of 48 cro...
Autores principales: | , , , |
---|---|
Formato: | Online Artículo Texto |
Lenguaje: | English |
Publicado: |
BioMed Central
2023
|
Materias: | |
Acceso en línea: | https://www.ncbi.nlm.nih.gov/pmc/articles/PMC10394804/ https://www.ncbi.nlm.nih.gov/pubmed/37528379 http://dx.doi.org/10.1186/s12903-023-03254-x |
_version_ | 1785083450607271936 |
---|---|
author | Delikan, Ebru Çaliskan, Seçil Çalışkan, Ahmet Özdemir, Canan |
author_facet | Delikan, Ebru Çaliskan, Seçil Çalışkan, Ahmet Özdemir, Canan |
author_sort | Delikan, Ebru |
collection | PubMed |
description | BACKGROUND: Since the effects of sterilization on the Fiberglass Reinforced Resin Crowns (FRRCs) is not well-known the aim of current study was to evaluate the effects of autoclave sterilization on the fracture resistance, color stability, and surface composition of FRRCs. METHODS: A total of 48 crowns were used. The crowns were divided into three groups according to the sterilization number: no sterilization (Control Group), one sterilization (Group 1), and four sterilizations (Group 2). The microstructure of the three crowns from each group was evaluated using scanning electron microscopy (SEM) and energy-dispersive X-ray (EDX) spectroscopy. Thirteen FRRCs from each group were first used for color stability testing and then for the fracture resistance analysis. One-way analysis of variance (ANOVA), one-way repeated measures ANOVA, and paired t-tests were used in the statistical analysis. RESULTS: EDX results revealed that the weight% of surface silicon atoms in group 2 was significantly higher. Some crack lines could be observed on the SEM images. Statistically significant differences were found in color stability following the first and fourth sterilization cycles (p < .01). The increase in the sterilization cycle did not statistically decrease the fracture resistance of the FRRCs (p = .055); however, overall, a decreasing trend was observed in fracture resistance as the sterilization cycle increased. CONCLUSIONS: Autoclave sterilization caused some changes in the surface elemental composition and surface morphology of FRRCs. Avoiding unnecessary FRRC trials is important to reduce the number of sterilizations. |
format | Online Article Text |
id | pubmed-10394804 |
institution | National Center for Biotechnology Information |
language | English |
publishDate | 2023 |
publisher | BioMed Central |
record_format | MEDLINE/PubMed |
spelling | pubmed-103948042023-08-03 Does repeated autoclave sterilization cause changes in the color and fragility of fiberglass reinforced resin crowns? Delikan, Ebru Çaliskan, Seçil Çalışkan, Ahmet Özdemir, Canan BMC Oral Health Research BACKGROUND: Since the effects of sterilization on the Fiberglass Reinforced Resin Crowns (FRRCs) is not well-known the aim of current study was to evaluate the effects of autoclave sterilization on the fracture resistance, color stability, and surface composition of FRRCs. METHODS: A total of 48 crowns were used. The crowns were divided into three groups according to the sterilization number: no sterilization (Control Group), one sterilization (Group 1), and four sterilizations (Group 2). The microstructure of the three crowns from each group was evaluated using scanning electron microscopy (SEM) and energy-dispersive X-ray (EDX) spectroscopy. Thirteen FRRCs from each group were first used for color stability testing and then for the fracture resistance analysis. One-way analysis of variance (ANOVA), one-way repeated measures ANOVA, and paired t-tests were used in the statistical analysis. RESULTS: EDX results revealed that the weight% of surface silicon atoms in group 2 was significantly higher. Some crack lines could be observed on the SEM images. Statistically significant differences were found in color stability following the first and fourth sterilization cycles (p < .01). The increase in the sterilization cycle did not statistically decrease the fracture resistance of the FRRCs (p = .055); however, overall, a decreasing trend was observed in fracture resistance as the sterilization cycle increased. CONCLUSIONS: Autoclave sterilization caused some changes in the surface elemental composition and surface morphology of FRRCs. Avoiding unnecessary FRRC trials is important to reduce the number of sterilizations. BioMed Central 2023-08-01 /pmc/articles/PMC10394804/ /pubmed/37528379 http://dx.doi.org/10.1186/s12903-023-03254-x Text en © The Author(s) 2023 https://creativecommons.org/licenses/by/4.0/Open Access This article is licensed under a Creative Commons Attribution 4.0 International License, which permits use, sharing, adaptation, distribution and reproduction in any medium or format, as long as you give appropriate credit to the original author(s) and the source, provide a link to the Creative Commons licence, and indicate if changes were made. The images or other third party material in this article are included in the article’s Creative Commons licence, unless indicated otherwise in a credit line to the material. If material is not included in the article’s Creative Commons licence and your intended use is not permitted by statutory regulation or exceeds the permitted use, you will need to obtain permission directly from the copyright holder. To view a copy of this licence, visit http://creativecommons.org/licenses/by/4.0/ (https://creativecommons.org/licenses/by/4.0/) . The Creative Commons Public Domain Dedication waiver (http://creativecommons.org/publicdomain/zero/1.0/ (https://creativecommons.org/publicdomain/zero/1.0/) ) applies to the data made available in this article, unless otherwise stated in a credit line to the data. |
spellingShingle | Research Delikan, Ebru Çaliskan, Seçil Çalışkan, Ahmet Özdemir, Canan Does repeated autoclave sterilization cause changes in the color and fragility of fiberglass reinforced resin crowns? |
title | Does repeated autoclave sterilization cause changes in the color and fragility of fiberglass reinforced resin crowns? |
title_full | Does repeated autoclave sterilization cause changes in the color and fragility of fiberglass reinforced resin crowns? |
title_fullStr | Does repeated autoclave sterilization cause changes in the color and fragility of fiberglass reinforced resin crowns? |
title_full_unstemmed | Does repeated autoclave sterilization cause changes in the color and fragility of fiberglass reinforced resin crowns? |
title_short | Does repeated autoclave sterilization cause changes in the color and fragility of fiberglass reinforced resin crowns? |
title_sort | does repeated autoclave sterilization cause changes in the color and fragility of fiberglass reinforced resin crowns? |
topic | Research |
url | https://www.ncbi.nlm.nih.gov/pmc/articles/PMC10394804/ https://www.ncbi.nlm.nih.gov/pubmed/37528379 http://dx.doi.org/10.1186/s12903-023-03254-x |
work_keys_str_mv | AT delikanebru doesrepeatedautoclavesterilizationcausechangesinthecolorandfragilityoffiberglassreinforcedresincrowns AT caliskansecil doesrepeatedautoclavesterilizationcausechangesinthecolorandfragilityoffiberglassreinforcedresincrowns AT calıskanahmet doesrepeatedautoclavesterilizationcausechangesinthecolorandfragilityoffiberglassreinforcedresincrowns AT ozdemircanan doesrepeatedautoclavesterilizationcausechangesinthecolorandfragilityoffiberglassreinforcedresincrowns |