Ceramic transition metal diboride superlattices with improved ductility and fracture toughness screened by ab initio calculations

Inherent brittleness, which easily leads to crack formation and propagation during use, is a serious problem for protective ceramic thin-film applications. Superlattice architectures, with alternating nm-thick layers of typically softer/stiffer materials, have been proven powerful method to improve...

Descripción completa

Detalles Bibliográficos
Autores principales: Fiantok, Tomáš, Koutná, Nikola, Sangiovanni, Davide G., Mikula, Marián
Formato: Online Artículo Texto
Lenguaje:English
Publicado: Nature Publishing Group UK 2023
Materias:
Acceso en línea:https://www.ncbi.nlm.nih.gov/pmc/articles/PMC10409783/
https://www.ncbi.nlm.nih.gov/pubmed/37553523
http://dx.doi.org/10.1038/s41598-023-39997-4
Descripción
Sumario:Inherent brittleness, which easily leads to crack formation and propagation during use, is a serious problem for protective ceramic thin-film applications. Superlattice architectures, with alternating nm-thick layers of typically softer/stiffer materials, have been proven powerful method to improve the mechanical performance of, e.g., cubic transition metal nitride ceramics. Using high-throughput first-principles calculations, we propose that superlattice structures hold promise also for enhancing mechanical properties and fracture resistance of transition metal diborides with two competing hexagonal phases, [Formula: see text] and [Formula: see text] . We study 264 possible combinations of [Formula: see text] , [Formula: see text] or [Formula: see text] MB[Formula: see text] (where M [Formula: see text] Al or group 3–6 transition metal) diboride superlattices. Based on energetic stability considerations, together with restrictions for lattice and shear modulus mismatch ([Formula: see text] , [Formula: see text]  GPa), we select 33 superlattice systems for further investigations. The identified systems are analysed in terms of mechanical stability and elastic constants, [Formula: see text] , where the latter provide indication of in-plane vs. out-of-plane strength ([Formula: see text] , [Formula: see text] ) and ductility ([Formula: see text] , [Formula: see text] ). The superlattice ability to resist brittle cleavage along interfaces is estimated by Griffith’s formula for fracture toughness. The [Formula: see text] -type TiB[Formula: see text] /MB[Formula: see text] (M [Formula: see text] Mo, W), HfB[Formula: see text] /WB[Formula: see text] , VB[Formula: see text] /MB[Formula: see text] (M [Formula: see text] Cr, Mo), NbB[Formula: see text] /MB[Formula: see text] (M [Formula: see text] Mo, W), and [Formula: see text] -type AlB[Formula: see text] /MB[Formula: see text] (M [Formula: see text] Nb, Ta, Mo, W), are suggested as the most promising candidates providing atomic-scale basis for enhanced toughness and resistance to crack growth.