Effect of Modifier Form on Mechanical Properties of Hypoeutectic Silumin

Aluminum–silicon alloys require modification due to their coarse-grained microstructures and resulting low strength properties. So far, research into the modification process has focused on the use of various chemical components and technological processes, the tasks of which are to refine the micro...

Descripción completa

Detalles Bibliográficos
Autor principal: Lipiński, Tomasz
Formato: Online Artículo Texto
Lenguaje:English
Publicado: MDPI 2023
Materias:
Acceso en línea:https://www.ncbi.nlm.nih.gov/pmc/articles/PMC10420200/
https://www.ncbi.nlm.nih.gov/pubmed/37569955
http://dx.doi.org/10.3390/ma16155250
_version_ 1785088719020097536
author Lipiński, Tomasz
author_facet Lipiński, Tomasz
author_sort Lipiński, Tomasz
collection PubMed
description Aluminum–silicon alloys require modification due to their coarse-grained microstructures and resulting low strength properties. So far, research into the modification process has focused on the use of various chemical components and technological processes, the tasks of which are to refine the microstructure and, thus, increase the mechanical properties of the alloy. In this paper, the answer to the question of whether the form of the modifier influences the modification effect of the hypoeutectic silumin will be found. The tests were carried out using the popular silumin AlSi7Mg. To answer our research question, the alloy was modified under comparable conditions using the following elements: Ti, B, and master alloys AlTi1.5 and AlB1.5. Modifiers in the form of Sr and master alloy AlSr1.5 were also used. All mentioned modifiers were produced and introduced into the liquid alloy in the form of a powder and a rod. Master alloys AlSr1.5 were also produced via cooling from the liquid state through cooling in air and the second variant at a speed of 200 °C/s (in the form of powder and a thin strip). The microstructure and mechanical properties were analyzed based on the following measures: tensile strength, elongation, and hardness of silumin. Based on the conducted research, it was found that the form of the modifier also affects the modification effect visible in the form of changes in the microstructure and mechanical properties. For the powder-modified alloy, greater fineness in the eutectic phase (α and B phases) and an increase in all analyzed mechanical properties were obtained.
format Online
Article
Text
id pubmed-10420200
institution National Center for Biotechnology Information
language English
publishDate 2023
publisher MDPI
record_format MEDLINE/PubMed
spelling pubmed-104202002023-08-12 Effect of Modifier Form on Mechanical Properties of Hypoeutectic Silumin Lipiński, Tomasz Materials (Basel) Article Aluminum–silicon alloys require modification due to their coarse-grained microstructures and resulting low strength properties. So far, research into the modification process has focused on the use of various chemical components and technological processes, the tasks of which are to refine the microstructure and, thus, increase the mechanical properties of the alloy. In this paper, the answer to the question of whether the form of the modifier influences the modification effect of the hypoeutectic silumin will be found. The tests were carried out using the popular silumin AlSi7Mg. To answer our research question, the alloy was modified under comparable conditions using the following elements: Ti, B, and master alloys AlTi1.5 and AlB1.5. Modifiers in the form of Sr and master alloy AlSr1.5 were also used. All mentioned modifiers were produced and introduced into the liquid alloy in the form of a powder and a rod. Master alloys AlSr1.5 were also produced via cooling from the liquid state through cooling in air and the second variant at a speed of 200 °C/s (in the form of powder and a thin strip). The microstructure and mechanical properties were analyzed based on the following measures: tensile strength, elongation, and hardness of silumin. Based on the conducted research, it was found that the form of the modifier also affects the modification effect visible in the form of changes in the microstructure and mechanical properties. For the powder-modified alloy, greater fineness in the eutectic phase (α and B phases) and an increase in all analyzed mechanical properties were obtained. MDPI 2023-07-26 /pmc/articles/PMC10420200/ /pubmed/37569955 http://dx.doi.org/10.3390/ma16155250 Text en © 2023 by the author. https://creativecommons.org/licenses/by/4.0/Licensee MDPI, Basel, Switzerland. This article is an open access article distributed under the terms and conditions of the Creative Commons Attribution (CC BY) license (https://creativecommons.org/licenses/by/4.0/).
spellingShingle Article
Lipiński, Tomasz
Effect of Modifier Form on Mechanical Properties of Hypoeutectic Silumin
title Effect of Modifier Form on Mechanical Properties of Hypoeutectic Silumin
title_full Effect of Modifier Form on Mechanical Properties of Hypoeutectic Silumin
title_fullStr Effect of Modifier Form on Mechanical Properties of Hypoeutectic Silumin
title_full_unstemmed Effect of Modifier Form on Mechanical Properties of Hypoeutectic Silumin
title_short Effect of Modifier Form on Mechanical Properties of Hypoeutectic Silumin
title_sort effect of modifier form on mechanical properties of hypoeutectic silumin
topic Article
url https://www.ncbi.nlm.nih.gov/pmc/articles/PMC10420200/
https://www.ncbi.nlm.nih.gov/pubmed/37569955
http://dx.doi.org/10.3390/ma16155250
work_keys_str_mv AT lipinskitomasz effectofmodifierformonmechanicalpropertiesofhypoeutecticsilumin