Cargando…
Enhanced Degradability, Mechanical Properties, and Flame Retardation of Poly(Lactic Acid) Composite with New Zealand Jade (Pounamu) Particles
Plastic pollution has become a global concern, demanding urgent attention and concerted efforts to mitigate its environmental impacts. Biodegradable plastics have emerged as a potential solution, offering the prospect of reduced harm through degradation over time. However, the lower mechanical stren...
Autores principales: | , , |
---|---|
Formato: | Online Artículo Texto |
Lenguaje: | English |
Publicado: |
MDPI
2023
|
Materias: | |
Acceso en línea: | https://www.ncbi.nlm.nih.gov/pmc/articles/PMC10421446/ https://www.ncbi.nlm.nih.gov/pubmed/37571164 http://dx.doi.org/10.3390/polym15153270 |
_version_ | 1785088982418194432 |
---|---|
author | Lin, Lilian Dang, Quang A. Park, Heon E. |
author_facet | Lin, Lilian Dang, Quang A. Park, Heon E. |
author_sort | Lin, Lilian |
collection | PubMed |
description | Plastic pollution has become a global concern, demanding urgent attention and concerted efforts to mitigate its environmental impacts. Biodegradable plastics have emerged as a potential solution, offering the prospect of reduced harm through degradation over time. However, the lower mechanical strength and slower degradation process of biodegradable plastics have hindered their widespread adoption. In this study, we investigate the incorporation of New Zealand (NZ) jade (pounamu) particles into poly(lactic acid) (PLA) to enhance the performance of the resulting composite. We aim to improve mechanical strength, flame retardation, and degradability. The material properties and compatibility with 3D printing technology were examined through a series of characterization techniques, including X-ray diffraction, dispersive X-ray fluorescence spectrometry, scanning electron microscopy, energy-dispersive X-ray spectroscopy, thermogravimetric analysis, 3D printing, compression molding, pycnometry, rheometry, tensile tests, three-point bending, and flammability testing. Our findings demonstrate that the addition of NZ jade particles significantly affects the density, thermal stability, and mechanical properties of the composites. Compounding NZ jade shows two different changes in thermal stability. It reduces flammability suggesting potential flame-retardant properties, and it accelerates the thermal degradation process as observed from the thermogravimetric analysis and the inferred decrease in molecular weight through rheometry. Thus, the presence of jade particles can also have the potential to enhance biodegradation, although further research is needed to assess its impact. The mechanical properties differ between compression-molded and 3D-printed samples, with compression-molded composites exhibiting higher strength and stiffness. Increasing jade content in composites further enhances their mechanical performance. Th results of this study contribute to the development of sustainable solutions for plastic pollution, paving the way for innovative applications and a cleaner environment. |
format | Online Article Text |
id | pubmed-10421446 |
institution | National Center for Biotechnology Information |
language | English |
publishDate | 2023 |
publisher | MDPI |
record_format | MEDLINE/PubMed |
spelling | pubmed-104214462023-08-12 Enhanced Degradability, Mechanical Properties, and Flame Retardation of Poly(Lactic Acid) Composite with New Zealand Jade (Pounamu) Particles Lin, Lilian Dang, Quang A. Park, Heon E. Polymers (Basel) Article Plastic pollution has become a global concern, demanding urgent attention and concerted efforts to mitigate its environmental impacts. Biodegradable plastics have emerged as a potential solution, offering the prospect of reduced harm through degradation over time. However, the lower mechanical strength and slower degradation process of biodegradable plastics have hindered their widespread adoption. In this study, we investigate the incorporation of New Zealand (NZ) jade (pounamu) particles into poly(lactic acid) (PLA) to enhance the performance of the resulting composite. We aim to improve mechanical strength, flame retardation, and degradability. The material properties and compatibility with 3D printing technology were examined through a series of characterization techniques, including X-ray diffraction, dispersive X-ray fluorescence spectrometry, scanning electron microscopy, energy-dispersive X-ray spectroscopy, thermogravimetric analysis, 3D printing, compression molding, pycnometry, rheometry, tensile tests, three-point bending, and flammability testing. Our findings demonstrate that the addition of NZ jade particles significantly affects the density, thermal stability, and mechanical properties of the composites. Compounding NZ jade shows two different changes in thermal stability. It reduces flammability suggesting potential flame-retardant properties, and it accelerates the thermal degradation process as observed from the thermogravimetric analysis and the inferred decrease in molecular weight through rheometry. Thus, the presence of jade particles can also have the potential to enhance biodegradation, although further research is needed to assess its impact. The mechanical properties differ between compression-molded and 3D-printed samples, with compression-molded composites exhibiting higher strength and stiffness. Increasing jade content in composites further enhances their mechanical performance. Th results of this study contribute to the development of sustainable solutions for plastic pollution, paving the way for innovative applications and a cleaner environment. MDPI 2023-08-01 /pmc/articles/PMC10421446/ /pubmed/37571164 http://dx.doi.org/10.3390/polym15153270 Text en © 2023 by the authors. https://creativecommons.org/licenses/by/4.0/Licensee MDPI, Basel, Switzerland. This article is an open access article distributed under the terms and conditions of the Creative Commons Attribution (CC BY) license (https://creativecommons.org/licenses/by/4.0/). |
spellingShingle | Article Lin, Lilian Dang, Quang A. Park, Heon E. Enhanced Degradability, Mechanical Properties, and Flame Retardation of Poly(Lactic Acid) Composite with New Zealand Jade (Pounamu) Particles |
title | Enhanced Degradability, Mechanical Properties, and Flame Retardation of Poly(Lactic Acid) Composite with New Zealand Jade (Pounamu) Particles |
title_full | Enhanced Degradability, Mechanical Properties, and Flame Retardation of Poly(Lactic Acid) Composite with New Zealand Jade (Pounamu) Particles |
title_fullStr | Enhanced Degradability, Mechanical Properties, and Flame Retardation of Poly(Lactic Acid) Composite with New Zealand Jade (Pounamu) Particles |
title_full_unstemmed | Enhanced Degradability, Mechanical Properties, and Flame Retardation of Poly(Lactic Acid) Composite with New Zealand Jade (Pounamu) Particles |
title_short | Enhanced Degradability, Mechanical Properties, and Flame Retardation of Poly(Lactic Acid) Composite with New Zealand Jade (Pounamu) Particles |
title_sort | enhanced degradability, mechanical properties, and flame retardation of poly(lactic acid) composite with new zealand jade (pounamu) particles |
topic | Article |
url | https://www.ncbi.nlm.nih.gov/pmc/articles/PMC10421446/ https://www.ncbi.nlm.nih.gov/pubmed/37571164 http://dx.doi.org/10.3390/polym15153270 |
work_keys_str_mv | AT linlilian enhanceddegradabilitymechanicalpropertiesandflameretardationofpolylacticacidcompositewithnewzealandjadepounamuparticles AT dangquanga enhanceddegradabilitymechanicalpropertiesandflameretardationofpolylacticacidcompositewithnewzealandjadepounamuparticles AT parkheone enhanceddegradabilitymechanicalpropertiesandflameretardationofpolylacticacidcompositewithnewzealandjadepounamuparticles |