Cargando…

Durability of GFRP and CFRP Bars in the Pore Solution of Calcium Sulfoaluminate Cement Concrete Made with Fresh or Seawater

Calcium sulfoaluminate cement concrete (CSAC) reinforced by fiber-reinforced polymer (FRP) bars, termed bars for brevity, is a good alternative to steel-reinforced concrete in marine environments due to the corrosion resistance of FRP and the lower pH of CSAC. For the first time, multi-mechanical te...

Descripción completa

Detalles Bibliográficos
Autores principales: Wang, Tuanjie, Razaqpur, Abdul Ghani, Chen, Shaoliang
Formato: Online Artículo Texto
Lenguaje:English
Publicado: MDPI 2023
Materias:
Acceso en línea:https://www.ncbi.nlm.nih.gov/pmc/articles/PMC10422602/
https://www.ncbi.nlm.nih.gov/pubmed/37571199
http://dx.doi.org/10.3390/polym15153306
_version_ 1785089251416735744
author Wang, Tuanjie
Razaqpur, Abdul Ghani
Chen, Shaoliang
author_facet Wang, Tuanjie
Razaqpur, Abdul Ghani
Chen, Shaoliang
author_sort Wang, Tuanjie
collection PubMed
description Calcium sulfoaluminate cement concrete (CSAC) reinforced by fiber-reinforced polymer (FRP) bars, termed bars for brevity, is a good alternative to steel-reinforced concrete in marine environments due to the corrosion resistance of FRP and the lower pH of CSAC. For the first time, multi-mechanical tests are conducted to compare the durability of glass FRP (GFRP) to that of carbon FRP (CFRP) after exposure to CSAC pore solution. The bars were immersed in a simulated pore solution of CSAC made with either fresh water and river sand or with seawater and sea sand. Solution temperature was held constant at 30 °C, 45 °C or 60 °C for 30, 60, 90 and 180 days of immersion. Tensile, horizontal and transverse shear tests, as well as detailed microstructural analyses, were conducted to determine the level and mechanisms of degradation for each type of bar. Sea salt increases the degradation of both bars, but it degrades GFRP more than CFRP. The bars’ retained tensile strength is a reliable indicator of their durability, while their post-exposure horizontal and transverse shear strengths are found inconsistent and counter intuitive. In the GFRP, the fiber, the epoxy matrix and their interface suffered damage, but in the CFRP, the carbon fiber was not damaged. Under the test conditions in this study, the maximum reduction in the tensile strength of the GFRP was 56.9% while that of CFRP was 15.1%. Based on the relevant ASTM standard, the CFRP bar satisfies the alkaline resistance requirement of the standard in the CSAC pore solution with and without salt, whereas the GFRP bar does not meet the same requirement in the above pore solution with salt.
format Online
Article
Text
id pubmed-10422602
institution National Center for Biotechnology Information
language English
publishDate 2023
publisher MDPI
record_format MEDLINE/PubMed
spelling pubmed-104226022023-08-13 Durability of GFRP and CFRP Bars in the Pore Solution of Calcium Sulfoaluminate Cement Concrete Made with Fresh or Seawater Wang, Tuanjie Razaqpur, Abdul Ghani Chen, Shaoliang Polymers (Basel) Article Calcium sulfoaluminate cement concrete (CSAC) reinforced by fiber-reinforced polymer (FRP) bars, termed bars for brevity, is a good alternative to steel-reinforced concrete in marine environments due to the corrosion resistance of FRP and the lower pH of CSAC. For the first time, multi-mechanical tests are conducted to compare the durability of glass FRP (GFRP) to that of carbon FRP (CFRP) after exposure to CSAC pore solution. The bars were immersed in a simulated pore solution of CSAC made with either fresh water and river sand or with seawater and sea sand. Solution temperature was held constant at 30 °C, 45 °C or 60 °C for 30, 60, 90 and 180 days of immersion. Tensile, horizontal and transverse shear tests, as well as detailed microstructural analyses, were conducted to determine the level and mechanisms of degradation for each type of bar. Sea salt increases the degradation of both bars, but it degrades GFRP more than CFRP. The bars’ retained tensile strength is a reliable indicator of their durability, while their post-exposure horizontal and transverse shear strengths are found inconsistent and counter intuitive. In the GFRP, the fiber, the epoxy matrix and their interface suffered damage, but in the CFRP, the carbon fiber was not damaged. Under the test conditions in this study, the maximum reduction in the tensile strength of the GFRP was 56.9% while that of CFRP was 15.1%. Based on the relevant ASTM standard, the CFRP bar satisfies the alkaline resistance requirement of the standard in the CSAC pore solution with and without salt, whereas the GFRP bar does not meet the same requirement in the above pore solution with salt. MDPI 2023-08-04 /pmc/articles/PMC10422602/ /pubmed/37571199 http://dx.doi.org/10.3390/polym15153306 Text en © 2023 by the authors. https://creativecommons.org/licenses/by/4.0/Licensee MDPI, Basel, Switzerland. This article is an open access article distributed under the terms and conditions of the Creative Commons Attribution (CC BY) license (https://creativecommons.org/licenses/by/4.0/).
spellingShingle Article
Wang, Tuanjie
Razaqpur, Abdul Ghani
Chen, Shaoliang
Durability of GFRP and CFRP Bars in the Pore Solution of Calcium Sulfoaluminate Cement Concrete Made with Fresh or Seawater
title Durability of GFRP and CFRP Bars in the Pore Solution of Calcium Sulfoaluminate Cement Concrete Made with Fresh or Seawater
title_full Durability of GFRP and CFRP Bars in the Pore Solution of Calcium Sulfoaluminate Cement Concrete Made with Fresh or Seawater
title_fullStr Durability of GFRP and CFRP Bars in the Pore Solution of Calcium Sulfoaluminate Cement Concrete Made with Fresh or Seawater
title_full_unstemmed Durability of GFRP and CFRP Bars in the Pore Solution of Calcium Sulfoaluminate Cement Concrete Made with Fresh or Seawater
title_short Durability of GFRP and CFRP Bars in the Pore Solution of Calcium Sulfoaluminate Cement Concrete Made with Fresh or Seawater
title_sort durability of gfrp and cfrp bars in the pore solution of calcium sulfoaluminate cement concrete made with fresh or seawater
topic Article
url https://www.ncbi.nlm.nih.gov/pmc/articles/PMC10422602/
https://www.ncbi.nlm.nih.gov/pubmed/37571199
http://dx.doi.org/10.3390/polym15153306
work_keys_str_mv AT wangtuanjie durabilityofgfrpandcfrpbarsintheporesolutionofcalciumsulfoaluminatecementconcretemadewithfreshorseawater
AT razaqpurabdulghani durabilityofgfrpandcfrpbarsintheporesolutionofcalciumsulfoaluminatecementconcretemadewithfreshorseawater
AT chenshaoliang durabilityofgfrpandcfrpbarsintheporesolutionofcalciumsulfoaluminatecementconcretemadewithfreshorseawater