Origin and Evolution of Cracks in the Glaze Surface of a Ceramic during the Cooling Process
Because of the significant difference between the thermal expansion coefficients of ceramic blank and glaze, the glaze typically undergoes more pronounced shrinkage than the blank during ceramic cooling, which results in high stress concentrations and cracking. In this study, the mechanical mechanis...
Autores principales: | Chen, Tiantian, Gong, Bin, Tang, Chun’an |
---|---|
Formato: | Online Artículo Texto |
Lenguaje: | English |
Publicado: |
MDPI
2023
|
Materias: | |
Acceso en línea: | https://www.ncbi.nlm.nih.gov/pmc/articles/PMC10456388/ https://www.ncbi.nlm.nih.gov/pubmed/37629798 http://dx.doi.org/10.3390/ma16165508 |
Ejemplares similares
-
Radioactivity Measurements on Glazed Ceramic Surfaces
por: Hobbs, Thomas G.
Publicado: (2000) -
Degradation Processes of Medieval and Renaissance Glazed Ceramics
por: Kolářová, Mária, et al.
Publicado: (2022) -
Sol-Gel ceramic glazes with photocatalytic activity
por: Monrós, G., et al.
Publicado: (2022) -
Antibacterial persistence of hydrophobically glazed ceramic tiles
por: Kim, Jinho, et al.
Publicado: (2022) -
Standard Test Method for Lead and Cadmium Extracted from Glazed Ceramic Surfaces
por: American Society for Testing and Materials. Philadelphia
Publicado: (1994)