Fatigue Threshold R-Curves for Dental Lithium Disilicate Glass–Ceramics
Chemical and mechanical fatigue degradation in ceramic materials is generally inconspicuous yet ubiquitous, to the effect that clinical fractures still consist of the main cause of failure in all-ceramic restorations. Implications of this span wide, from a reduced survival prognosis for the affected...
Autores principales: | Lubauer, J., Lohbauer, U., Belli, R. |
---|---|
Formato: | Online Artículo Texto |
Lenguaje: | English |
Publicado: |
SAGE Publications
2023
|
Materias: | |
Acceso en línea: | https://www.ncbi.nlm.nih.gov/pmc/articles/PMC10467012/ https://www.ncbi.nlm.nih.gov/pubmed/37448337 http://dx.doi.org/10.1177/00220345231180565 |
Ejemplares similares
-
Effectiveness and safety of bleaching agents on lithium disilicate glass ceramics
por: Ozdogan, Alper, et al.
Publicado: (2022) -
Replacement of missing lateral incisors with lithium disilicate glass-ceramic veneer-fixed dental prostheses: a clinical report
por: Bissasu, Sami M, et al.
Publicado: (2014) -
Flexural strength and microstructure of two lithium disilicate glass ceramics for CAD/CAM restoration in the dental clinic
por: Kang, Suk-Ho, et al.
Publicado: (2013) -
Surface properties of a new lithium disilicate glass-ceramic after grinding
por: Miotto, Larissa Natiele, et al.
Publicado: (2021) -
Post-fatigue fracture load, stress concentration and mechanical properties of feldspathic, leucite- and lithium disilicate-reinforced glass ceramics
por: Capobianco, Vinicius, et al.
Publicado: (2023)