Standardizing critical current density measurements in lithium garnets
The formation of Li dendrites at the Li/electrolyte interface at practically relevant current densities (> 1 mA cm(−2)) is a critical issue hindering the deployment of non-flammable and non-toxic Li(7)La(3)Zr(2)O(12) (LLZO) electrolyte in solid-state batteries. In this comment, the authors argue...
Autores principales: | , , , |
---|---|
Formato: | Online Artículo Texto |
Lenguaje: | English |
Publicado: |
Nature Publishing Group UK
2023
|
Materias: | |
Acceso en línea: | https://www.ncbi.nlm.nih.gov/pmc/articles/PMC10492854/ https://www.ncbi.nlm.nih.gov/pubmed/37689811 http://dx.doi.org/10.1038/s42004-023-01002-4 |
Sumario: | The formation of Li dendrites at the Li/electrolyte interface at practically relevant current densities (> 1 mA cm(−2)) is a critical issue hindering the deployment of non-flammable and non-toxic Li(7)La(3)Zr(2)O(12) (LLZO) electrolyte in solid-state batteries. In this comment, the authors argue for an agreement to standardize measurements of the critical current density at which Li dendrites begin to penetrate the LLZO solid-state electrolyte. |
---|