Fiber Melt Spinning and Thermo-Stabilization of Para-Rubber Wood Lignin: An Approach for Fully Biomass Precursor Preparation
[Image: see text] Para-rubber wood (PRW) lignin, extracted from agricultural waste, was successfully melt-spun to fibers and thermo-stabilized without employing auxiliary additives. (31)P NMR analysis revealed that PRW-lignin contained mainly a syringyl unit of phenolic C(5)-substituted OH group, wh...
Autores principales: | , , , , , , , |
---|---|
Formato: | Online Artículo Texto |
Lenguaje: | English |
Publicado: |
American Chemical Society
2023
|
Acceso en línea: | https://www.ncbi.nlm.nih.gov/pmc/articles/PMC10515410/ https://www.ncbi.nlm.nih.gov/pubmed/37744868 http://dx.doi.org/10.1021/acsomega.3c04590 |
_version_ | 1785108941961691136 |
---|---|
author | Wannid, Prapudsorn Hararak, Bongkot Padee, Sirada Klinsukhon, Wattana Suwannamek, Natthaphop Raita, Marisa Champreda, Verawat Prahsarn, Chureerat |
author_facet | Wannid, Prapudsorn Hararak, Bongkot Padee, Sirada Klinsukhon, Wattana Suwannamek, Natthaphop Raita, Marisa Champreda, Verawat Prahsarn, Chureerat |
author_sort | Wannid, Prapudsorn |
collection | PubMed |
description | [Image: see text] Para-rubber wood (PRW) lignin, extracted from agricultural waste, was successfully melt-spun to fibers and thermo-stabilized without employing auxiliary additives. (31)P NMR analysis revealed that PRW-lignin contained mainly a syringyl unit of phenolic C(5)-substituted OH group, which enabled melt flow during fiber spinning, as well as a guaiacyl unit which offered the ability to cross-link during thermo-stabilization. Thermo-stabilized fibers with no fusion were achieved at 250 °C with the heating rate of 0.1 °C/min. Structural changes in the fibers during stabilization were systematically investigated using FTIR and XPS analyses. From the results, changes in the intensities of characteristic bands relating to C–H stretching, aromatic C–H stretching, and C=O stretching indicated structural changes of lignin toward aromaticity via oxidation reactions. XPS analysis of the fibers carbonized at 900, 1000, and 1200 °C revealed an increase in carbon content from 72 to 87 wt %. and a decrease in oxygen content from 28 to 13 wt %. with the increasing carbonization temperature. The weight loss of carbonized fibers was in the range of 73.6 to 88.7%. The high weight loss of fibers carbonized at 1200 °C was explained partly due to the thermal decomposition of disordered carbon. The tensile strength and modulus of carbonized fibers were 163.0 and 275.1 MPa, respectively. This study demonstrates an approach to prepare a fully biomass precursor fiber and contributes to the exploration of the potential use of lignin from biomass waste. |
format | Online Article Text |
id | pubmed-10515410 |
institution | National Center for Biotechnology Information |
language | English |
publishDate | 2023 |
publisher | American Chemical Society |
record_format | MEDLINE/PubMed |
spelling | pubmed-105154102023-09-23 Fiber Melt Spinning and Thermo-Stabilization of Para-Rubber Wood Lignin: An Approach for Fully Biomass Precursor Preparation Wannid, Prapudsorn Hararak, Bongkot Padee, Sirada Klinsukhon, Wattana Suwannamek, Natthaphop Raita, Marisa Champreda, Verawat Prahsarn, Chureerat ACS Omega [Image: see text] Para-rubber wood (PRW) lignin, extracted from agricultural waste, was successfully melt-spun to fibers and thermo-stabilized without employing auxiliary additives. (31)P NMR analysis revealed that PRW-lignin contained mainly a syringyl unit of phenolic C(5)-substituted OH group, which enabled melt flow during fiber spinning, as well as a guaiacyl unit which offered the ability to cross-link during thermo-stabilization. Thermo-stabilized fibers with no fusion were achieved at 250 °C with the heating rate of 0.1 °C/min. Structural changes in the fibers during stabilization were systematically investigated using FTIR and XPS analyses. From the results, changes in the intensities of characteristic bands relating to C–H stretching, aromatic C–H stretching, and C=O stretching indicated structural changes of lignin toward aromaticity via oxidation reactions. XPS analysis of the fibers carbonized at 900, 1000, and 1200 °C revealed an increase in carbon content from 72 to 87 wt %. and a decrease in oxygen content from 28 to 13 wt %. with the increasing carbonization temperature. The weight loss of carbonized fibers was in the range of 73.6 to 88.7%. The high weight loss of fibers carbonized at 1200 °C was explained partly due to the thermal decomposition of disordered carbon. The tensile strength and modulus of carbonized fibers were 163.0 and 275.1 MPa, respectively. This study demonstrates an approach to prepare a fully biomass precursor fiber and contributes to the exploration of the potential use of lignin from biomass waste. American Chemical Society 2023-09-06 /pmc/articles/PMC10515410/ /pubmed/37744868 http://dx.doi.org/10.1021/acsomega.3c04590 Text en © 2023 The Authors. Published by American Chemical Society https://creativecommons.org/licenses/by/4.0/Permits the broadest form of re-use including for commercial purposes, provided that author attribution and integrity are maintained (https://creativecommons.org/licenses/by/4.0/). |
spellingShingle | Wannid, Prapudsorn Hararak, Bongkot Padee, Sirada Klinsukhon, Wattana Suwannamek, Natthaphop Raita, Marisa Champreda, Verawat Prahsarn, Chureerat Fiber Melt Spinning and Thermo-Stabilization of Para-Rubber Wood Lignin: An Approach for Fully Biomass Precursor Preparation |
title | Fiber Melt Spinning
and Thermo-Stabilization of Para-Rubber
Wood Lignin: An Approach for Fully Biomass Precursor Preparation |
title_full | Fiber Melt Spinning
and Thermo-Stabilization of Para-Rubber
Wood Lignin: An Approach for Fully Biomass Precursor Preparation |
title_fullStr | Fiber Melt Spinning
and Thermo-Stabilization of Para-Rubber
Wood Lignin: An Approach for Fully Biomass Precursor Preparation |
title_full_unstemmed | Fiber Melt Spinning
and Thermo-Stabilization of Para-Rubber
Wood Lignin: An Approach for Fully Biomass Precursor Preparation |
title_short | Fiber Melt Spinning
and Thermo-Stabilization of Para-Rubber
Wood Lignin: An Approach for Fully Biomass Precursor Preparation |
title_sort | fiber melt spinning
and thermo-stabilization of para-rubber
wood lignin: an approach for fully biomass precursor preparation |
url | https://www.ncbi.nlm.nih.gov/pmc/articles/PMC10515410/ https://www.ncbi.nlm.nih.gov/pubmed/37744868 http://dx.doi.org/10.1021/acsomega.3c04590 |
work_keys_str_mv | AT wannidprapudsorn fibermeltspinningandthermostabilizationofpararubberwoodligninanapproachforfullybiomassprecursorpreparation AT hararakbongkot fibermeltspinningandthermostabilizationofpararubberwoodligninanapproachforfullybiomassprecursorpreparation AT padeesirada fibermeltspinningandthermostabilizationofpararubberwoodligninanapproachforfullybiomassprecursorpreparation AT klinsukhonwattana fibermeltspinningandthermostabilizationofpararubberwoodligninanapproachforfullybiomassprecursorpreparation AT suwannameknatthaphop fibermeltspinningandthermostabilizationofpararubberwoodligninanapproachforfullybiomassprecursorpreparation AT raitamarisa fibermeltspinningandthermostabilizationofpararubberwoodligninanapproachforfullybiomassprecursorpreparation AT champredaverawat fibermeltspinningandthermostabilizationofpararubberwoodligninanapproachforfullybiomassprecursorpreparation AT prahsarnchureerat fibermeltspinningandthermostabilizationofpararubberwoodligninanapproachforfullybiomassprecursorpreparation |