Transport limitations in polyolefin cracking at the single catalyst particle level
Catalytic cracking is a promising approach to chemically recycle polyolefins by converting them into smaller hydrocarbons like naphtha, and important precursors of various platform chemicals, such as aromatics. Cracking catalysts, commonly used in the modern refinery and petrochemical industry, are...
Autores principales: | , , , , , |
---|---|
Formato: | Online Artículo Texto |
Lenguaje: | English |
Publicado: |
The Royal Society of Chemistry
2023
|
Materias: | |
Acceso en línea: | https://www.ncbi.nlm.nih.gov/pmc/articles/PMC10529962/ https://www.ncbi.nlm.nih.gov/pubmed/37772101 http://dx.doi.org/10.1039/d3sc03229a |
_version_ | 1785111449773801472 |
---|---|
author | Rejman, Sebastian Vollmer, Ina Werny, Maximilian J. Vogt, Eelco T. C. Meirer, Florian Weckhuysen, Bert M. |
author_facet | Rejman, Sebastian Vollmer, Ina Werny, Maximilian J. Vogt, Eelco T. C. Meirer, Florian Weckhuysen, Bert M. |
author_sort | Rejman, Sebastian |
collection | PubMed |
description | Catalytic cracking is a promising approach to chemically recycle polyolefins by converting them into smaller hydrocarbons like naphtha, and important precursors of various platform chemicals, such as aromatics. Cracking catalysts, commonly used in the modern refinery and petrochemical industry, are tailored to process gaseous or liquid feedstock. Polyolefins, however, are very large macromolecules that form highly viscous melts at the temperatures required to break their backbone C–C bonds. Therefore, mass transport is expected to limit the performance of traditional cracking catalysts when applied to the conversion of polymers. In this work, we study these effects during the cracking of polypropylene (PP) over catalysts utilized in the fluid catalytic cracking (FCC) process. Thermogravimetric experiments using PP of varying molecular weight (M(w)) and catalysts of varying accessibility showed that low M(w) model polymers can be cracked below 275 °C, while PP of higher M(w) required a 150 °C higher temperature. We propose that this difference is linked to different degrees of mass transport limitations and investigated this at length scales ranging from milli- to nanometers, utilizing in situ optical microscopy and electron microscopy to inspect cut open catalyst–polymer composites. We identified the main cause of transport limitations as the significantly higher melt viscosity of high M(w) polymers, which prohibits efficient catalyst–polymer contact. Additionally, the high M(w) polymer does not enter the inner pore system of the catalyst particles, severely limiting utilization of the active sites located there. Our results demonstrate that utilizing low M(w) polymers can lead to a significant overestimation of catalyst activity, and suggest that polyolefins might need to undergo a viscosity reducing pre-treatment in order to be cracked efficiently. |
format | Online Article Text |
id | pubmed-10529962 |
institution | National Center for Biotechnology Information |
language | English |
publishDate | 2023 |
publisher | The Royal Society of Chemistry |
record_format | MEDLINE/PubMed |
spelling | pubmed-105299622023-09-28 Transport limitations in polyolefin cracking at the single catalyst particle level Rejman, Sebastian Vollmer, Ina Werny, Maximilian J. Vogt, Eelco T. C. Meirer, Florian Weckhuysen, Bert M. Chem Sci Chemistry Catalytic cracking is a promising approach to chemically recycle polyolefins by converting them into smaller hydrocarbons like naphtha, and important precursors of various platform chemicals, such as aromatics. Cracking catalysts, commonly used in the modern refinery and petrochemical industry, are tailored to process gaseous or liquid feedstock. Polyolefins, however, are very large macromolecules that form highly viscous melts at the temperatures required to break their backbone C–C bonds. Therefore, mass transport is expected to limit the performance of traditional cracking catalysts when applied to the conversion of polymers. In this work, we study these effects during the cracking of polypropylene (PP) over catalysts utilized in the fluid catalytic cracking (FCC) process. Thermogravimetric experiments using PP of varying molecular weight (M(w)) and catalysts of varying accessibility showed that low M(w) model polymers can be cracked below 275 °C, while PP of higher M(w) required a 150 °C higher temperature. We propose that this difference is linked to different degrees of mass transport limitations and investigated this at length scales ranging from milli- to nanometers, utilizing in situ optical microscopy and electron microscopy to inspect cut open catalyst–polymer composites. We identified the main cause of transport limitations as the significantly higher melt viscosity of high M(w) polymers, which prohibits efficient catalyst–polymer contact. Additionally, the high M(w) polymer does not enter the inner pore system of the catalyst particles, severely limiting utilization of the active sites located there. Our results demonstrate that utilizing low M(w) polymers can lead to a significant overestimation of catalyst activity, and suggest that polyolefins might need to undergo a viscosity reducing pre-treatment in order to be cracked efficiently. The Royal Society of Chemistry 2023-08-16 /pmc/articles/PMC10529962/ /pubmed/37772101 http://dx.doi.org/10.1039/d3sc03229a Text en This journal is © The Royal Society of Chemistry https://creativecommons.org/licenses/by/3.0/ |
spellingShingle | Chemistry Rejman, Sebastian Vollmer, Ina Werny, Maximilian J. Vogt, Eelco T. C. Meirer, Florian Weckhuysen, Bert M. Transport limitations in polyolefin cracking at the single catalyst particle level |
title | Transport limitations in polyolefin cracking at the single catalyst particle level |
title_full | Transport limitations in polyolefin cracking at the single catalyst particle level |
title_fullStr | Transport limitations in polyolefin cracking at the single catalyst particle level |
title_full_unstemmed | Transport limitations in polyolefin cracking at the single catalyst particle level |
title_short | Transport limitations in polyolefin cracking at the single catalyst particle level |
title_sort | transport limitations in polyolefin cracking at the single catalyst particle level |
topic | Chemistry |
url | https://www.ncbi.nlm.nih.gov/pmc/articles/PMC10529962/ https://www.ncbi.nlm.nih.gov/pubmed/37772101 http://dx.doi.org/10.1039/d3sc03229a |
work_keys_str_mv | AT rejmansebastian transportlimitationsinpolyolefincrackingatthesinglecatalystparticlelevel AT vollmerina transportlimitationsinpolyolefincrackingatthesinglecatalystparticlelevel AT wernymaximilianj transportlimitationsinpolyolefincrackingatthesinglecatalystparticlelevel AT vogteelcotc transportlimitationsinpolyolefincrackingatthesinglecatalystparticlelevel AT meirerflorian transportlimitationsinpolyolefincrackingatthesinglecatalystparticlelevel AT weckhuysenbertm transportlimitationsinpolyolefincrackingatthesinglecatalystparticlelevel |