Microstructure Evolution of the Ti-46Al-8Nb-2.5V Alloy during Hot Compression and Subsequent Annealing at 900 °C
TiAl alloys are high-temperature structural materials with excellent comprehensive properties, and their ideal service temperature range is about 700–950 °C. High-Nb containing the Ti-46Al-8Nb-2.5V alloy was subjected to hot compression and subsequent annealing at 900 °C. During hot compression, wor...
Autores principales: | Cao, Shouzhen, Li, Zongze, Pu, Jiafei, Han, Jianchao, Dong, Qi, Zhu, Mingdong |
---|---|
Formato: | Online Artículo Texto |
Lenguaje: | English |
Publicado: |
MDPI
2023
|
Materias: | |
Acceso en línea: | https://www.ncbi.nlm.nih.gov/pmc/articles/PMC10533025/ https://www.ncbi.nlm.nih.gov/pubmed/37763454 http://dx.doi.org/10.3390/ma16186176 |
Ejemplares similares
-
Quasi-In-Situ Analysis of As-Rolled Microstructure of Magnesium Alloys during Annealing and Subsequent Plastic Deformation
por: Deng, Jiafei, et al.
Publicado: (2022) -
Effects of Nb on the Microstructure and Compressive Properties of an As-Cast Ni(44)Ti(44)Nb(12) Eutectic Alloy
por: Liu, Shifeng, et al.
Publicado: (2019) -
Effect of Cold Drawing and Annealing in Thermomechanical Treatment Route on the Microstructure and Functional Properties of Superelastic Ti-Zr-Nb Alloy
por: Kudryashova, Anastasia, et al.
Publicado: (2023) -
Low Temperature Phase Transformations in Copper-Quenched Ti-44.5Al-8Nb-2.5V Alloy
por: Cao, Shouzhen, et al.
Publicado: (2017) -
Effect of Nb on the Microstructure, Mechanical Properties, Corrosion Behavior, and Cytotoxicity of Ti-Nb Alloys
por: Han, Mi-Kyung, et al.
Publicado: (2015)