Revealing the aging process of solid electrolyte interphase on SiO(x) anode

As one of the most promising alternatives to graphite negative electrodes, silicon oxide (SiO(x)) has been hindered by its fast capacity fading. Solid electrolyte interphase (SEI) aging on silicon SiO(x) has been recognized as the most critical yet least understood facet. Herein, leveraging 3D focus...

Descripción completa

Detalles Bibliográficos
Autores principales: Qian, Guoyu, Li, Yiwei, Chen, Haibiao, Xie, Lin, Liu, Tongchao, Yang, Ni, Song, Yongli, Lin, Cong, Cheng, Junfang, Nakashima, Naotoshi, Zhang, Meng, Li, Zikun, Zhao, Wenguang, Yang, Xiangjie, Lin, Hai, Lu, Xia, Yang, Luyi, Li, Hong, Amine, Khalil, Chen, Liquan, Pan, Feng
Formato: Online Artículo Texto
Lenguaje:English
Publicado: Nature Publishing Group UK 2023
Materias:
Acceso en línea:https://www.ncbi.nlm.nih.gov/pmc/articles/PMC10539371/
https://www.ncbi.nlm.nih.gov/pubmed/37770484
http://dx.doi.org/10.1038/s41467-023-41867-6
Descripción
Sumario:As one of the most promising alternatives to graphite negative electrodes, silicon oxide (SiO(x)) has been hindered by its fast capacity fading. Solid electrolyte interphase (SEI) aging on silicon SiO(x) has been recognized as the most critical yet least understood facet. Herein, leveraging 3D focused ion beam-scanning electron microscopy (FIB-SEM) tomographic imaging, we reveal an exceptionally characteristic SEI microstructure with an incompact inner region and a dense outer region, which overturns the prevailing belief that SEIs are homogeneous structure and reveals the SEI evolution process. Through combining nanoprobe and electron energy loss spectroscopy (EELS), it is also discovered that the electronic conductivity of thick SEI relies on the percolation network within composed of conductive agents (e.g., carbon black particles), which are embedded into the SEI upon its growth. Therefore, the free growth of SEI will gradually attenuate this electron percolation network, thereby causing capacity decay of SiO(x). Based on these findings, a proof-of-concept strategy is adopted to mechanically restrict the SEI growth via applying a confining layer on top of the electrode. Through shedding light on the fundamental understanding of SEI aging for SiO(x) anodes, this work could potentially inspire viable improving strategies in the future.