Effect of Hydrothermal Degradation on Flexural Fatigue Strength of Various Cubic-Containing Translucent Zirconia

Objective  The aim of this study is to investigate the fatigue and hydrothermal degradation behavior among the cubic-containing translucent yttrium oxide stabilized tetragonal zirconia polycrystal (Y-TZP). Materials and Methods  Four groups of commercial Y-TZP (T, ST, XT, and P), containing differen...

Descripción completa

Detalles Bibliográficos
Autores principales: Kengtanyakich, Santiphab, Peampring, Chaimongkon
Formato: Online Artículo Texto
Lenguaje:English
Publicado: Thieme Medical and Scientific Publishers Pvt. Ltd. 2022
Acceso en línea:https://www.ncbi.nlm.nih.gov/pmc/articles/PMC10569846/
https://www.ncbi.nlm.nih.gov/pubmed/36220117
http://dx.doi.org/10.1055/s-0042-1755630
_version_ 1785119631890972672
author Kengtanyakich, Santiphab
Peampring, Chaimongkon
author_facet Kengtanyakich, Santiphab
Peampring, Chaimongkon
author_sort Kengtanyakich, Santiphab
collection PubMed
description Objective  The aim of this study is to investigate the fatigue and hydrothermal degradation behavior among the cubic-containing translucent yttrium oxide stabilized tetragonal zirconia polycrystal (Y-TZP). Materials and Methods  Four groups of commercial Y-TZP (T, ST, XT, and P), containing different amount of cubic crystal, were examined. Artificial aging was accomplished by autoclaving at 122°C under 2 bar pressure for 8 hours. Fatigue simulation parameters were set using an axial 50 N load, a total of 240,000 cycles. Flexural fatigue strength was evaluated. Statistical Analysis  Two-way analysis of variance with Tukey's honestly significant difference test was used to determine the difference in fatigue strength values between various type of zirconia materials within control and aging with a significant level of 5%. Weibull analysis was conducted on the fatigue strength data. Results  All groups showed the mean flexural fatigue strength had no significant difference in hydrothermally aged specimens compared with specimens without aging ( p  = 0.154). Group T showed significantly higher flexural fatigue strength followed by group ST, XT, and P. Group XT and P showed no significant difference in strength value ( p  > 0.05). Group T demonstrated a lower probability of failure than group ST, XT, and P whether with or without aging. Weibull modulus in group T and ST with aging condition was increased and higher than all the experimental groups. Conclusion  Cubic-containing zirconia materials (group ST, XT, and P) exhibited lower flexural fatigue strength than non-cubic 3Y-TZP zirconia (group T). However, various cubic-containing translucent zirconia was assumed to have high resistance to hydrothermal degradation.
format Online
Article
Text
id pubmed-10569846
institution National Center for Biotechnology Information
language English
publishDate 2022
publisher Thieme Medical and Scientific Publishers Pvt. Ltd.
record_format MEDLINE/PubMed
spelling pubmed-105698462023-10-13 Effect of Hydrothermal Degradation on Flexural Fatigue Strength of Various Cubic-Containing Translucent Zirconia Kengtanyakich, Santiphab Peampring, Chaimongkon Eur J Dent Objective  The aim of this study is to investigate the fatigue and hydrothermal degradation behavior among the cubic-containing translucent yttrium oxide stabilized tetragonal zirconia polycrystal (Y-TZP). Materials and Methods  Four groups of commercial Y-TZP (T, ST, XT, and P), containing different amount of cubic crystal, were examined. Artificial aging was accomplished by autoclaving at 122°C under 2 bar pressure for 8 hours. Fatigue simulation parameters were set using an axial 50 N load, a total of 240,000 cycles. Flexural fatigue strength was evaluated. Statistical Analysis  Two-way analysis of variance with Tukey's honestly significant difference test was used to determine the difference in fatigue strength values between various type of zirconia materials within control and aging with a significant level of 5%. Weibull analysis was conducted on the fatigue strength data. Results  All groups showed the mean flexural fatigue strength had no significant difference in hydrothermally aged specimens compared with specimens without aging ( p  = 0.154). Group T showed significantly higher flexural fatigue strength followed by group ST, XT, and P. Group XT and P showed no significant difference in strength value ( p  > 0.05). Group T demonstrated a lower probability of failure than group ST, XT, and P whether with or without aging. Weibull modulus in group T and ST with aging condition was increased and higher than all the experimental groups. Conclusion  Cubic-containing zirconia materials (group ST, XT, and P) exhibited lower flexural fatigue strength than non-cubic 3Y-TZP zirconia (group T). However, various cubic-containing translucent zirconia was assumed to have high resistance to hydrothermal degradation. Thieme Medical and Scientific Publishers Pvt. Ltd. 2022-10-11 /pmc/articles/PMC10569846/ /pubmed/36220117 http://dx.doi.org/10.1055/s-0042-1755630 Text en The Author(s). This is an open access article published by Thieme under the terms of the Creative Commons Attribution License, permitting unrestricted use, distribution, and reproduction so long as the original work is properly cited. ( https://creativecommons.org/licenses/by/4.0/ ) https://creativecommons.org/licenses/by/4.0/This is an open-access article distributed under the terms of the Creative Commons Attribution License, which permits unrestricted use, distribution, and reproduction in any medium, provided the original work is properly cited.
spellingShingle Kengtanyakich, Santiphab
Peampring, Chaimongkon
Effect of Hydrothermal Degradation on Flexural Fatigue Strength of Various Cubic-Containing Translucent Zirconia
title Effect of Hydrothermal Degradation on Flexural Fatigue Strength of Various Cubic-Containing Translucent Zirconia
title_full Effect of Hydrothermal Degradation on Flexural Fatigue Strength of Various Cubic-Containing Translucent Zirconia
title_fullStr Effect of Hydrothermal Degradation on Flexural Fatigue Strength of Various Cubic-Containing Translucent Zirconia
title_full_unstemmed Effect of Hydrothermal Degradation on Flexural Fatigue Strength of Various Cubic-Containing Translucent Zirconia
title_short Effect of Hydrothermal Degradation on Flexural Fatigue Strength of Various Cubic-Containing Translucent Zirconia
title_sort effect of hydrothermal degradation on flexural fatigue strength of various cubic-containing translucent zirconia
url https://www.ncbi.nlm.nih.gov/pmc/articles/PMC10569846/
https://www.ncbi.nlm.nih.gov/pubmed/36220117
http://dx.doi.org/10.1055/s-0042-1755630
work_keys_str_mv AT kengtanyakichsantiphab effectofhydrothermaldegradationonflexuralfatiguestrengthofvariouscubiccontainingtranslucentzirconia
AT peampringchaimongkon effectofhydrothermaldegradationonflexuralfatiguestrengthofvariouscubiccontainingtranslucentzirconia