Green Synthesis of NiFe(2)O(4) Nano-Spinel Oxide-Decorated Carbon Nanotubes for Efficient Capacitive Performance—Effect of Electrolyte Concentration
Energy storage applications received great attention due to environmental aspects. A green method was used to prepare a composite of nickel–iron-based spinel oxide nanoparticle@CNT. The prepared materials were characterized by different analytical methods like X-ray diffraction, X-ray photon spectro...
Autores principales: | , , , , , |
---|---|
Formato: | Online Artículo Texto |
Lenguaje: | English |
Publicado: |
MDPI
2023
|
Materias: | |
Acceso en línea: | https://www.ncbi.nlm.nih.gov/pmc/articles/PMC10574157/ https://www.ncbi.nlm.nih.gov/pubmed/37836284 http://dx.doi.org/10.3390/nano13192643 |
Sumario: | Energy storage applications received great attention due to environmental aspects. A green method was used to prepare a composite of nickel–iron-based spinel oxide nanoparticle@CNT. The prepared materials were characterized by different analytical methods like X-ray diffraction, X-ray photon spectroscopy (XPS), scanning electron microscopy (SEM), and transmitted electron microscopy (TEM). The synergistic effect between nickel–iron oxide and carbon nanotubes was characterized using different electrochemical methods like cyclic voltammetry (CV), galvanostatic charging/discharging (GCD), and electrochemical impedance spectroscopy (EIS). The capacitances of the pristine NiFe(2)O(4) and NiFe(2)O(4)@CNT were studied in different electrolyte concentrations. The effect of [Formula: see text] concentrations was studied for modified and non-modified surfaces. Furthermore, the specific capacitance was estimated for pristine and modified NiFe(2)O(4) at a wide current range (5 to 17 A g(−1)). Thus, the durability of different surfaces after 2000 cycles was studied, and the capacitance retention was estimated as 78.8 and 90.1% for pristine and modified NiFe(2)O(4). On the other hand, the capacitance rate capability was observed as 65.1% (5 to 17 A g(−1)) and 62.4% (5 to 17 A g(−1)) for NiFe(2)O(4) and NiFe(2)O(4)@CNT electrodes. |
---|